产品中心

Akulon® F-X9215

Akulon® F-X9215

产品产商:帝斯曼(DSM)
产品产地:欧洲/中国
产品类别:聚酰胺6PA6
产品型号:Akulon F-X9215
产品规格:25KG/
产品特性:低粘度、热稳定性、中等粘性

Akulon® F-X9215

聚酰胺6
产品说明:
Low/Medium Viscosity

Special Features:
  • Heat stabilized or stable to heat

  • Low viscosity

  • Medium viscosity


Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

添加剂
  • 热稳定剂

特性
  • 低粘度、热稳定性、中等粘性
加工方法
  • 注射成型

树脂ID (ISO 1043)
  • PA6

物理性能
干燥
调节后的
单位制
测试方法
密度
1.13
--
g/cm³
ISO 1183
吸水率



ISO 62
饱和, 73°F
9.5
--
%

平衡, 73°F, 50% RH
2.5
--
%

粘数
162
--
cm³/g
ISO 307
机械性能
干燥
调节后的
单位制
测试方法
拉伸模量
290000
--
psi
ISO 527-2
拉伸应力 (屈服)
8700
--
psi
ISO 527-2
拉伸应变 (屈服)
8.0
--
%
ISO 527-2
标称拉伸断裂应变
> 50
--
%
ISO 527-2
冲击性能
干燥
调节后的
单位制
测试方法
简支梁缺口冲击强度 (73°F)
3.3
--
ft·lb/in²
ISO 179/1eA
简支梁无缺口冲击强度 (73°F)
无断裂
无断裂

ISO 179/1eU
热性能
干燥
调节后的
单位制
测试方法
熔融温度 2
428
--
°F
ISO 11357-3
线形热膨胀系数



ISO 11359-2
流动
5.0E-5
--
in/in/°F

横向
5.6E-5
--
in/in/°F

注射
干燥
单位制

干燥温度
176
°F

干燥时间
4.0 到 8.0
hr

料筒后部温度
446 到 455
°F

料筒中部温度
455 到 482
°F

料筒前部温度
464 到 500
°F

射嘴温度
464 到 518
°F

加工(熔体)温度
464 到 527
°F

模具温度
122 到 176
°F

注射速度
中等偏快


背压
435 到 1450
psi

螺杆压缩比
2.5:1.0



如需帝斯曼原厂物性表及相关文件,请联系我们工作人员,谢谢!