Desmopan® 5080A
热塑性聚氨酯弹性体(酯/醚)
injection molding grade; improved microbial resistance; Improved hydrolysis resistance; Application; Seals, membranes; hard to soft systems
密度 |
|
|
|
73°F | 1.14 | g/cm³ | ISO 1183 |
-- | 0.0412 | lb/in³ | ISO 1183 3 |
肖氏硬度 |
|
|
|
邵氏 A, 1 秒, 73°F | 80 |
| ISO 7619 |
邵氏 D, 1 秒, 73°F | 29 |
| ISO 7619 |
邵氏 A, 3 sec | 80 |
| ISO 868 3 |
邵氏 D, 15 sec | 29 |
| ISO 868 3 |
拉伸应力 4 |
|
| DIN 53504 |
断裂, 73°F | 3450 | psi |
|
10% 应变, 73°F | 218 | psi |
|
50% 应变, 73°F | 551 | psi |
|
100% 应变, 73°F | 725 | psi |
|
300% 应变, 73°F | 1250 | psi |
|
拉伸应变 4 (断裂, 73°F) | 700 | % | DIN 53504 |
Tensile Storage Modulus |
|
| ISO 6721 |
-4°F | 15229 | psi |
|
68°F | 4496 | psi |
|
140°F | 3336 | psi |
|
抗磨损性 5 | 70.0 | mm³ | ISO 4649 |
撕裂强度 6 (73°F) | 310 | lbf/in | ISO 34-1 |
压缩永久变形 |
|
| ISO 815 |
73°F, 72 hr | 20 | % |
|
158°F, 24 hr 5 | 24 | % |
|
158°F, 24 hr 7 | 19 | % |
|
Rebound Resilience | 45 | % | ISO 4662 |
干燥温度 | < 176 | °F |
|
加工(熔体)温度 | 374 到 410 | °F |
|
模具温度 | 68 到 104 | °F |
|