Stanyl® TW350
聚酰胺 46
产品说明:
Heat Stabilized, Flame Retardant
Special Features:
Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.
添加剂 | |
特性 | |
加工方法 | |
树脂ID (ISO 1043) | |
密度 | 1.39 | g/cm³ | ISO 1183 |
收缩率 |
|
| ISO 294-4 |
横向流量 | 1.5 | % |
|
流量 | 1.5 | % |
|
吸水率 |
|
| ISO 62 |
饱和, 73°F | 8.5 | % |
|
平衡, 73°F, 50% RH | 2.4 | % |
|
拉伸模量 | 493000 | psi | ISO 527-2 |
拉伸应力 (屈服) | 11600 | psi | ISO 527-2 |
拉伸应变 (屈服) | 4.5 | % | ISO 527-2 |
标称拉伸断裂应变 | 20 | % | ISO 527-2 |
弯曲模量 | 464000 | psi | ISO 178 |
简支梁缺口冲击强度 |
|
| ISO 179/1eA |
-22°F | 1.9 | ft·lb/in² |
|
73°F | 2.9 | ft·lb/in² |
|
热变形温度 (264 psi, 未退火) | 374 | °F | ISO 75-2/A |
玻璃转化温度 3 | 167 | °F | ISO 11357-2 |
熔融温度 3 | 563 | °F | ISO 11357-3 |
线形热膨胀系数 |
|
| ISO 11359-2 |
流动 | 4.4E-5 | in/in/°F |
|
横向 | 5.0E-5 | in/in/°F |
|
RTI Elec (0.030 in) | 284 | °F | UL 746 |
可燃性等级 (0.06 in) | V-0 |
| IEC 60695-11-10, -20 |
极限氧指数 | 29 | % | ISO 4589-2 |
熔体密度 | 1.14 | g/cm³ |
|
熔体导热性 | 1.7 | Btu·in/hr/ft²/°F |
|
干燥温度 | 176 | °F |
干燥时间 | 4.0 到 8.0 | hr |
料筒后部温度 | 536 到 608 | °F |
料筒中部温度 | 572 到 608 | °F |
料筒前部温度 | 572 到 608 | °F |
射嘴温度 | 572 到 608 | °F |
加工(熔体)温度 | 590 到 608 | °F |
模具温度 | 176 到 248 | °F |
注射速度 | 中等偏快 |
|
背压 | 290 到 1450 | psi |
螺杆压缩比 | 2.5:1.0 |
|
如需恩骅力(Envalior)原厂物性表及相关文件,请联系我司工作人员,谢谢!