Stanyl® TS250F4D
聚酰胺 46
产品说明:
20% Glass Reinforced, Flame Retardant, Heat Stabilized, Improved resistance to blistering during reflow - soldering process
Special Features:
Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.
填料/增强材料 | |
添加剂 | |
特性 | |
加工方法 | |
树脂ID (ISO 1043) | |
密度 | 1.60 | -- | g/cm³ | ISO 1183 |
收缩率 |
|
|
| ISO 294-4 |
横向流量 | 1.3 | -- | % |
|
流量 | 0.80 | -- | % |
|
吸水率 |
|
|
| ISO 62 |
饱和, 73°F | 6.3 | -- | % |
|
平衡, 73°F, 50% RH | 1.7 | -- | % |
|
粘数 | 145 | -- | cm³/g | ISO 307 |
拉伸模量 | 1.33E+6 | 870000 | psi | ISO 527-2 |
拉伸应力 (断裂) | 21800 | 14500 | psi | ISO 527-2 |
拉伸应变 (断裂) | 2.5 | 4.0 | % | ISO 527-2 |
简支梁缺口冲击强度 |
|
|
| ISO 179/1eA |
-22°F | 3.8 | 3.8 | ft·lb/in² |
|
73°F | 4.8 | 4.8 | ft·lb/in² |
|
热变形温度 |
|
|
|
|
66 psi, 未退火 | 554 | -- | °F | ISO 75-2/B |
264 psi, 未退火 | 554 | -- | °F | ISO 75-2/A |
玻璃转化温度 3 | 167 | -- | °F | ISO 11357-2 |
维卡软化温度 | 554 | -- | °F | ISO 306/B50 |
熔融温度 3 | 563 | -- | °F | ISO 11357-3 |
线形热膨胀系数 |
|
|
| ISO 11359-2 |
流动 | 2.2E-5 | -- | in/in/°F |
|
横向 | 3.3E-5 | -- | in/in/°F |
|
RTI Elec (0.026 in) | 266 | -- | °F | UL 746 |
体积电阻率 | > 1.0E+15 | 1.0E+10 | ohms·cm | IEC 60093 |
介电强度 | 760 | 510 | V/mil | IEC 60243-1 |
相对电容率 |
|
|
| IEC 60250 |
100 Hz | 4.30 | -- |
|
|
1 MHz | 4.00 | -- |
|
|
耗散因数 |
|
|
| IEC 60250 |
100 Hz | 6.0E-3 | 0.33 |
|
|
1 MHz | 0.016 | 0.070 |
|
|
漏电起痕指数 | 200 | -- | V | IEC 60112 |
可燃性等级 |
|
|
| IEC 60695-11-10, -20 |
0.026 in | V-0 | -- |
|
|
0.06 in | V-0 | -- |
|
|
干燥温度 | 176 | °F |
干燥时间 | 4.0 到 8.0 | hr |
料筒后部温度 | 536 到 608 | °F |
料筒中部温度 | 572 到 608 | °F |
料筒前部温度 | 572 到 608 | °F |
射嘴温度 | 572 到 608 | °F |
加工(熔体)温度 | 581 到 608 | °F |
模具温度 | 176 到 248 | °F |
注射速度 | 中等偏快 |
|
背压 | 290 到 1450 | psi |
螺杆压缩比 | 2.5:1.0 |
|
如需恩骅力(Envalior)原厂物性表及相关文件,请联系我司工作人员,谢谢!