Stanyl® TE250F6
聚酰胺 46
产品说明:
30% Glass Reinforced, Heat Stabilized, Flame Retardant
Special Features:
Used In:
Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.
填料/增强材料 | |
添加剂 | |
特性 | |
用途 | |
机构评级 | |
加工方法 | |
多点数据 | Isochronous Stress vs. Strain (ISO 11403-1) Isothermal Stress vs. Strain (ISO 11403-1) Secant Modulus vs. Strain (ISO 11403-1) Shear Modulus vs. Temperature (ISO 11403-1) Viscosity vs. Shear Rate (ISO 11403-2)
|
树脂ID (ISO 1043) | |
密度 | 1.68 | -- | g/cm³ | ISO 1183 |
收缩率 |
|
|
| ISO 294-4 |
横向流量 | 1.1 | -- | % |
|
流量 | 0.40 | -- | % |
|
吸水率 |
|
|
| ISO 62 |
饱和, 73°F | 5.9 | -- | % |
|
平衡, 73°F, 50% RH | 1.6 | -- | % |
|
粘数 | 145 | -- | cm³/g | ISO 307 |
拉伸模量 |
|
|
| ISO 527-2 |
-- | 1.74E+6 | 1.16E+6 | psi |
|
248°F | 1.09E+6 | -- | psi |
|
320°F | 899000 | -- | psi |
|
拉伸应力 |
|
|
| ISO 527-2 |
断裂 | 26100 | 18100 | psi |
|
断裂, 248°F | 15200 | -- | psi |
|
断裂, 320°F | 13800 | -- | psi |
|
拉伸应变 |
|
|
| ISO 527-2 |
断裂 | 2.5 | 3.5 | % |
|
断裂, 248°F | 4.0 | -- | % |
|
断裂, 320°F | 4.0 | -- | % |
|
弯曲模量 |
|
|
| ISO 178 |
-- | 1.60E+6 | 1.06E+6 | psi |
|
248°F | 943000 | -- | psi |
|
320°F | 725000 | -- | psi |
|
简支梁缺口冲击强度 |
|
|
| ISO 179/1eA |
-22°F | 4.8 | 4.8 | ft·lb/in² |
|
73°F | 5.2 | 5.2 | ft·lb/in² |
|
简支梁无缺口冲击强度 |
|
|
| ISO 179/1eU |
-22°F | 24 | 24 | ft·lb/in² |
|
73°F | 29 | 29 | ft·lb/in² |
|
悬壁梁缺口冲击强度 |
|
|
| ISO 180/1A |
-40°F | 5.2 | 5.2 | ft·lb/in² |
|
73°F | 5.2 | 5.2 | ft·lb/in² |
|
热变形温度 |
|
|
|
|
66 psi, 未退火 | 554 | -- | °F | ISO 75-2/B |
264 psi, 未退火 | 554 | -- | °F | ISO 75-2/A |
玻璃转化温度 3 | 167 | -- | °F | ISO 11357-2 |
维卡软化温度 | 554 | -- | °F | ISO 306/B50 |
熔融温度 3 | 563 | -- | °F | ISO 11357-3 |
线形热膨胀系数 |
|
|
| ISO 11359-2 |
流动 | 1.4E-5 | -- | in/in/°F |
|
横向 | 3.1E-5 | -- | in/in/°F |
|
RTI Elec (0.030 in) | 284 | -- | °F | UL 746 |
Effective Thermal Diffusivity | 1.59E-7 | -- | m²/s |
|
Thermal Index - 5000 hr | 325 | -- | °F | IEC 60216 |
干燥温度 | 176 | °F |
干燥时间 | 4.0 到 8.0 | hr |
料筒后部温度 | 536 到 608 | °F |
料筒中部温度 | 572 到 608 | °F |
料筒前部温度 | 572 到 608 | °F |
射嘴温度 | 572 到 608 | °F |
加工(熔体)温度 | 581 到 608 | °F |
模具温度 | 176 到 248 | °F |
注射速度 | 中等偏快 |
|
背压 | 290 到 1450 | psi |
螺杆压缩比 | 2.5:1.0 |
|
如需恩骅力(Envalior)原厂物性表及相关文件,请联系我司工作人员,谢谢!