Products

Zytel® ST7301 NC010

Zytel® ST7301 NC010

Manufacturer: DUPONT
Produced At:
 Import/ China
Product Category: NYLON 6/PA6
Product No:
 Zytel ST7301 NC010
Product Quantity: 25KG / BAG
Product Features:
 Heat Stabilized

Zytel® ST7301 NC010

NYLON RESIN
Product Description:
Super Toughened Polyamide 6

Additive 
  • Heat StabilizerLubricantMold Release
Features 
  • Heat Stabilized

RoHS Compliance 
  • Contact Manufacturer

Forms 
  • Pellets

Processing Method 
  • CastingCoatingExtrusionFilm ExtrusionInjection MoldingProfile ExtrusionSheet Extrusion
Multi-Point Data 
  • Isothermal Stress vs. Strain (ISO 11403-1)Secant Modulus vs. Strain (ISO 11403-1)Shear Stress vs. Shear Rate (ISO 11403-1)Specific Volume vs Temperature (ISO 11403-2)Viscosity vs. Shear Rate (ISO 11403-2)
Part Marking Code (ISO 11469)
  • PA6-HI

Resin ID (ISO 1043)
  • PA6-HI

Physical
Dry
Conditioned
Unit
Test Method
Density
1.06
--
g/cm³
ISO 1183
Molding Shrinkage



ISO 294-4
Across Flow
1.0
--
%

Across Flow : 176°F, 48 hr
0.10
--
%

Flow
1.0
--
%

Flow : 176°F, 48 hr
0.10
--
%

Water Absorption (Equilibrium, 73°F, 0.0787 in, 50% RH)
2.7
--
%
ISO 62
Viscosity Number (96% H2SO4 (Sulphuric Acid))
160
--
cm³/g
ISO 307
Hardness
Dry
Conditioned
Unit
Test Method
Ball Indentation Hardness 2 (H 358/30)
13800
--
psi
ISO 2039-1
Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
261000
79800
psi
ISO 527-2
Tensile Stress (Yield)
6960
4210
psi
ISO 527-2
Tensile Strain (Yield)
4.0
30
%
ISO 527-2
Nominal Tensile Strain at Break
> 50
> 50
%
ISO 527-2
Flexural Modulus
247000
79800
psi
ISO 178
Flexural Stress (3.5% Strain)
7690
4640
psi
ISO 178
Poisson's Ratio
0.41
0.47

ISO 527
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-40°F
8.6
8.1
ft·lb/in²

-22°F
8.1
8.6
ft·lb/in²

73°F
38
57
ft·lb/in²

Charpy Unnotched Impact Strength



ISO 179/1eU
-22°F
No Break
No Break


73°F
No Break
No Break


Notched Izod Impact Strength



ISO 180/1A
-40°F
7.1
6.2
ft·lb/in²

-22°F
6.7
7.1
ft·lb/in²

73°F
29
45
ft·lb/in²

Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature




66 psi, Unannealed
203
--
°F
ISO 75-2/B
264 psi, Unannealed
124
--
°F
ISO 75-2/A
Melting Temperature 3
430
--
°F
ISO 11357-3
Flammability
Dry
Conditioned
Unit
Test Method
Burning Rate 4 (0.0394 in)
< 3.9
--
in/min
ISO 3795
FMVSS Flammability
B
--

FMVSS 302
Fill Analysis
Dry
Conditioned
Unit

Melt Density
0.960
--
g/cm³

Specific Heat Capacity of Melt
0.621
--
Btu/lb/°F

Thermal Conductivity of Melt
1.0
--
Btu·in/hr/ft²/°F

Injection
Dry
Unit

Drying Temperature
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Suggested Max Moisture
0.20
%

Processing (Melt) Temp
500 to 536
°F

Melt Temperature, Optimum
518
°F

Mold Temperature
122 to 194
°F

Mold Temperature, Optimum
158
°F

Holding Pressure
7250 to 14500
psi

Drying Recommended
yes


Hold Pressure Time
4.00
s/mm

Maximum Screw Tangential Speed
709
in/min



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation
展开