Products

Zytel® 73G30T NC010

Zytel® 73G30T NC010

Manufacturer: DUPONT
Produced At:
 Import/ China
Product Category: NYLON 6/PA6
Product No:
 Zytel 73G30T NC010
Product Quantity: 25KG / BAG

Zytel® 73G30T NC010

NYLON RESIN
Product Description:
30% Glass Reinforced, Toughened, Polyamide 6

Filler / Reinforcement 
  • Glass Fiber, 30% Filler by Weight

Additive 
  • Mold Release

RoHS Compliance 
  • Contact Manufacturer

Forms 
  • Pellets

Processing Method 
  • Injection Molding

Multi-Point Data 
  • Isothermal Stress vs. Strain (ISO 11403-1)

  • Secant Modulus vs. Strain (ISO 11403-1)

  • Shear Modulus vs. Temperature (ISO 11403-1)

  • Shear Modulus vs. Temperature, Dynamic (ISO 11403-1)

  • Shear Stress vs. Shear Rate (ISO 11403-1)

  • Specific Volume vs Temperature (ISO 11403-2)

  • Viscosity vs. Shear Rate (ISO 11403-2)

Part Marking Code (ISO 11469)
  • PA6-IGF30

Resin ID (ISO 1043)
  • PA6-IGF30

Physical
Dry
Conditioned
Unit
Test Method
Density
1.34
--
g/cm³
ISO 1183
Molding Shrinkage



ISO 294-4
Across Flow
1.0
--
%

Flow
0.20
--
%

Water Absorption



ISO 62
Saturation, 73°F, 0.0787 in
6.2
--
%

Equilibrium, 73°F, 0.0787 in, 50% RH
1.8
--
%

Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
1.32E+6
827000
psi
ISO 527-2
Tensile Stress (Break)
24700
16000
psi
ISO 527-2
Tensile Strain (Break)
3.0
6.0
%
ISO 527-2
Flexural Modulus
1.31E+6
827000
psi
ISO 178
Poisson's Ratio
0.34
0.35

ISO 527
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-22°F
6.2
5.7
ft·lb/in²

73°F
9.5
12
ft·lb/in²

Charpy Unnotched Impact Strength



ISO 179/1eU
-22°F
48
45
ft·lb/in²

73°F
48
48
ft·lb/in²

Notched Izod Impact Strength



ISO 180/1A
-22°F
5.7
5.7
ft·lb/in²

73°F
8.1
11
ft·lb/in²

Unnotched Izod Impact Strength(73°F)
38
38
ft·lb/in²
ISO 180/1U
Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature




66 psi, Unannealed
430
--
°F
ISO 75-2/B
264 psi, Unannealed
410
--
°F
ISO 75-2/A
Vicat Softening Temperature
419
--
°F
ISO 306/B50
Melting Temperature 3
430
--
°F
ISO 11357-3
CLTE



ISO 11359-2
Flow
1.6E-5
--
in/in/°F

Transverse
6.7E-5
--
in/in/°F

Electrical
Dry
Conditioned
Unit
Test Method
Comparative Tracking Index
550
--
V
IEC 60112
Flammability
Dry
Conditioned
Unit
Test Method
Burning Rate 4 (0.0394 in)
0.87
--
in/min
ISO 3795
Flame Rating (0.06 in)
HB
--

UL 94, IEC 60695-11-10, -20
FMVSS Flammability
B
--

FMVSS 302
Fill Analysis
Dry
Conditioned
Unit
Test Method
Melt Density
1.31
--
g/cm³

Specific Heat Capacity of Melt
0.526
--
Btu/lb/°F

Thermal Conductivity of Melt
1.6
--
Btu·in/hr/ft²/°F

Additional Information
Dry
Conditioned
Unit
Test Method
Odor
3.50
--

VDA 270
Injection
Dry
Unit

Drying Temperature
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Suggested Max Moisture
0.20
%

Processing (Melt) Temp
500 to 536
°F

Melt Temperature, Optimum
518
°F

Mold Temperature
122 to 212
°F

Mold Temperature, Optimum
176
°F

Holding Pressure
7250 to 14500
psi

Drying Recommended
yes


Hold Pressure Time
3.00
s/mm

Maximum Screw Tangential Speed
472
in/min



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields