Products

Zytel® 73G30T BK261

Zytel® 73G30T BK261

Manufacturer: DUPONT
Produced At:
 Import/ China
Product Category: NYLON 6/PA6
Product No:
 Zytel 73G30T BK261
Product Quantity: 25KG / BAG

Zytel® 73G30T BK261

NYLON RESIN
Product Description:
30% Glass Reinforced, Toughened, Polyamide 6

Filler / Reinforcement 
  • Glass Fiber, 30% Filler by Weight

RoHS Compliance 
  • Contact Manufacturer

Processing Method 
  • Injection Molding

Multi-Point Data 
  • Tensile Modulus vs. Temperature, Dynamic (ISO 11403-1)

Part Marking Code (ISO 11469)
  • PA6-IGF30

Resin ID (ISO 1043)
  • PA6-IGF30

Physical
Dry
Conditioned
Unit
Test Method
Density
1.34
--
g/cm³
ISO 1183
Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
1.36E+6
812000
psi
ISO 527-2
Tensile Stress (Break)
24700
16000
psi
ISO 527-2
Tensile Strain (Break)
3.0
6.0
%
ISO 527-2
Flexural Modulus
1.31E+6
827000
psi
ISO 178
Poisson's Ratio
0.34
0.35

ISO 527
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-22°F
4.8
4.8
ft·lb/in²

73°F
8.6
12
ft·lb/in²

Charpy Unnotched Impact Strength(73°F)
45
45
ft·lb/in²
ISO 179/1eU
Notched Izod Impact Strength



ISO 180/1A
-22°F
5.2
5.2
ft·lb/in²

73°F
8.1
10
ft·lb/in²

Unnotched Izod Impact Strength(73°F)
36
36
ft·lb/in²
ISO 180/1U
Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
403
--
°F
ISO 75-2/A
Melting Temperature 3
430
--
°F
ISO 11357-3
CLTE



ISO 11359-2
Flow
2.2E-6
--
in/in/°F

Flow : -40 to 73°F
1.4E-5
--
in/in/°F

Flow : 131 to 320°F
3.3E-6
--
in/in/°F

Transverse
6.1E-5
--
in/in/°F

Transverse : -40 to 73°F
4.7E-5
--
in/in/°F

Transverse : 131 to 320°F
6.1E-5
--
in/in/°F

Flammability
Dry
Conditioned
Unit
Test Method
Burning Rate 4 (0.0394 in)
0.87
--
in/min
ISO 3795
Flame Rating (0.06 in)
HB
--

UL 94, IEC 60695-11-10, -20
FMVSS Flammability
B
--

FMVSS 302
Additional Information
Dry
Conditioned

Test Method
Odor
3.50
--

VDA 270
Injection
Dry
Unit

Drying Temperature
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Suggested Max Moisture
0.20
%

Processing (Melt) Temp
500 to 536
°F

Melt Temperature, Optimum
518
°F

Mold Temperature
122 to 212
°F

Mold Temperature, Optimum
176
°F

Holding Pressure
7250 to 14500
psi

Drying Recommended
yes


Hold Pressure Time
3.00
s/mm

Maximum Screw Tangential Speed
472
in/min



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation
展开