Products

Zytel® 73G30HSL NC010

Zytel® 73G30HSL NC010

Manufacturer: DUPONT
Produced At:
 Import/ China
Product Category: NYLON 6/PA6
Product No:
 Zytel 73G30HSL NC010
Product Quantity: 25KG / BAG
Product Features:
 Heat Stabilized

Zytel® 73G30HSL NC010

NYLON RESIN
Product Description:
30% Glass Reinforced, Heat Stabilized, Polyamide 6

Filler / Reinforcement 
  • Glass Fiber, 30% Filler by Weight

Additive 
  • Heat Stabilizer,Lubricant,Mold Release
Features 
  • Heat Stabilized

RoHS Compliance 
  • Contact Manufacturer

Forms 
  • Pellets

Processing Method 
  • Injection Molding

Multi-Point Data 
  • Coefficient of Thermal Expansion vs. Temperature (ISO 11403-1)

  • Creep Modulus vs. Time (ISO 11403-1)

  • Isochronous Stress vs. Strain (ISO 11403-1)

  • Isothermal Stress vs. Strain (ISO 11403-1)

  • Secant Modulus vs. Strain (ISO 11403-1)

  • Shear Stress vs. Shear Rate (ISO 11403-1)

  • Specific Volume vs Temperature (ISO 11403-2)

  • Tensile Fatigue (Wöhler) (ISO 11403-2)

  • Tensile Modulus vs. Temperature (ISO 11403-1)

  • Viscosity vs. Shear Rate (ISO 11403-2)

Part Marking Code (ISO 11469)
  • PA6-GF30

Resin ID (ISO 1043)
  • PA6-GF30

Physical
Dry
Conditioned
Unit
Test Method
Density
1.36
--
g/cm³
ISO 1183
Molding Shrinkage



ISO 294-4
Across Flow
0.60
--
%

Flow
0.20
--
%

Water Absorption



ISO 62
Saturation, 73°F, 0.0787 in
6.3
--
%

Equilibrium, 73°F, 0.0787 in, 50% RH
1.9
--
%

Hardness
Dry
Conditioned
Unit
Test Method
Rockwell Hardness (R-Scale)
121
--

ISO 2039-2
Ball Indentation Hardness (H 961/30)
33400
21800
psi
ISO 2039-1
Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
1.38E+6
870000
psi
ISO 527-2
Tensile Stress (Break)
27600
17400
psi
ISO 527-2
Tensile Strain (Break)
3.5
6.0
%
ISO 527-2
Tensile Creep Modulus



ISO 899-1
1 hr
--
798000
psi

1000 hr
--
653000
psi

Flexural Modulus 3
1.23E+6
798000
psi
ISO 178
Flexural Stress 3
40600
26100
psi
ISO 178
Poisson's Ratio
0.34
0.35

ISO 527
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-22°F
4.8
10
ft·lb/in²

73°F
7.6
11
ft·lb/in²

Charpy Unnotched Impact Strength



ISO 179/1eU
-22°F
38
38
ft·lb/in²

73°F
48
48
ft·lb/in²

Notched Izod Impact Strength



ISO 180/1A
-22°F
4.8
5.2
ft·lb/in²

73°F
7.1
9.5
ft·lb/in²

Unnotched Izod Impact Strength (73°F)
38
--
ft·lb/in²
ISO 180/1U
Multi-Axial Instrumented Impact Energy(73°F)
2.58
4.79
ft·lb
ISO 6603-2
Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature




66 psi, Unannealed
428
--
°F
ISO 75-2/B
264 psi, Unannealed
410
--
°F
ISO 75-2/A
Glass Transition Temperature 4
140
--
°F
ISO 11357-2
Vicat Softening Temperature
419
--
°F
ISO 306/B50
Melting Temperature 4
430
--
°F
ISO 11357-3
CLTE



ISO 11359-2
Flow
1.4E-5
--
in/in/°F

Transverse
4.2E-5
--
in/in/°F

Effective Thermal Diffusivity
9.10E-8
--
m²/s

Flammability
Dry
Conditioned
Unit
Test Method
Burning Rate 5 (0.0394 in)
2.0
--
in/min
ISO 3795
Flame Rating



UL 94, IEC 60695-11-10, -20
0.030 in
HB
--


0.06 in
HB
--


Oxygen Index 6
21
--
%
ISO 4589-2
FMVSS Flammability
B
--

FMVSS 302
Fogging



ISO 6452
F-value (refraction)
95
--
%

G-value (condensate)
1.0E-4
--
g

Fill Analysis
Dry
Conditioned
Unit
Test Method
Melt Density
1.20
--
g/cm³

Specific Heat Capacity of Melt
0.545
--
Btu/lb/°F

Thermal Conductivity of Melt
1.8
--
Btu·in/hr/ft²/°F

Additional Information
Dry
Conditioned
Unit
Test Method
Emission of Organic Compounds
8.50
--
µgC/g
VDA 277
Odor
3.50
--

VDA 270
Injection
Dry
Unit

Drying Temperature
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Suggested Max Moisture
0.20
%

Processing (Melt) Temp
500 to 536
°F

Melt Temperature, Optimum
518
°F

Mold Temperature
158 to 248
°F

Mold Temperature, Optimum
212
°F

Holding Pressure
7250 to 14500

Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation