Products

Delrin® 150 NC010

Delrin® 150 NC010

Manufacturer: DUPONT
Produced At:
 Import/ China
Product Category: POM
Product No:
 Delrin 150 NC010
Product Quantity: 25KG / BAG
Product Features:
 High ViscosityHomopolymerNucleated

Delrin® 150 NC010

ACETAL RESIN
Product Description:
Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion

Additive 
  • Mold Release,Nucleating Agent 
Features 
  • High Viscosity,Homopolymer,Nucleated
RoHS Compliance 
  • Contact Manufacturer

Forms 
  • Pellets

Processing Method 
  • ExtrusionInjection MoldingProfile ExtrusionSheet Extrusion 
Multi-Point Data 
  • Isothermal Stress vs. Strain (ISO 11403-1)Secant Modulus vs. Strain (ISO 11403-1) 
Part Marking Code (ISO 11469)
  • POM

Resin ID (ISO 1043)
  • POM

Physical
Nominal Value
Unit
Test Method
Density
1.42
g/cm³
ISO 1183
Melt Mass-Flow Rate (MFR)
2.4
g/10 min
ISO 1133
Melt Volume-Flow Rate (MVR) (190°C/2.16 kg)
0.116
in³/10min
ISO 1133
Molding Shrinkage


ISO 294-4
Across Flow
2.0
%

Flow
1.8
%

Hardness
Nominal Value
Unit
Test Method
Rockwell Hardness


ISO 2039-2
M-Scale
94


R-Scale
122


Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
450000
psi
ISO 527-2
Tensile Stress (Yield)
10400
psi
ISO 527-2
Tensile Strain (Yield)
22
%
ISO 527-2
Nominal Tensile Strain at Break
40
%
ISO 527-2
Flexural Modulus
421000
psi
ISO 178
Poisson's Ratio
0.37

ISO 527
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength


ISO 179/1eA
-22°F
4.3
ft·lb/in²

73°F
5.7
ft·lb/in²

Notched Izod Impact Strength (73°F)
4.8
ft·lb/in²
ISO 180/1A
Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature



66 psi, Unannealed
329
°F
ISO 75-2/B
264 psi, Unannealed
207
°F
ISO 75-2/A
Melting Temperature 3
352
°F
ISO 11357-3
CLTE


ISO 11359-2
Flow
6.1E-5
in/in/°F

Flow : -40 to 73°F
3.9E-7
in/in/°F

Flow : 131 to 320°F
7.8E-7
in/in/°F

Transverse
5.6E-5
in/in/°F

Transverse : -40 to 73°F
5.0E-7
in/in/°F

Transverse : 131 to 320°F
8.9E-7
in/in/°F

Annealing Temperature
320
°F

Annealing Time - Optional
30.0
min/mm

Flammability
Nominal Value
Unit
Test Method
Burning Rate 4 (0.0394 in)
< 3.9
in/min
ISO 3795
Flame Rating (0.06 in)
HB

UL 94, IEC 60695-11-10, -20
FMVSS Flammability
B

FMVSS 302
Additional Information
Nominal Value
Unit
Test Method
Emission
< 8.00
mg/kg
VDA 275
Injection
Nominal Value
Unit

Drying Temperature
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Suggested Max Moisture
0.20
%

Processing (Melt) Temp
410 to 428
°F

Melt Temperature, Optimum
419
°F

Mold Temperature
176 to 212
°F

Mold Temperature, Optimum
194
°F

Holding Pressure
13100 to 16000
psi

Drying Recommended
yes


Hold Pressure Time
7.50
s/mm

Extrusion
Nominal Value
Unit

Drying Temperature
167 to 185
°F

Drying Time
2.0 to 4.0
hr

Suggested Max Moisture
0.20
%

Melt Temperature
383 to 401
°F

Extrusion Melt Temperature, Optimum
392
°F



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation
展开