Thermoplastic Copolyester Elastomer
Product Description:
Blow Molding Grade

Special Features:
  • Heat stabilized or stable to heat


Used In:
  • Boots and Bellows


Arnitel® is a high-performance ThermoPlastic Copolyester (TPC) that offers you a unique combination of flexibility, high temperature resistance and strength - plus excellent processing characteristics.
In industries ranging from automotive to E&E, Arnitel® is increasingly being as a lighter, smarter, greener alternative to conventional rubbers €" reducing environmental impact and ultimately, system costs.
The product is supported by an experienced and knowledgeable global team continuously working on new ideas and applications, as well as exploring new markets. By listening to your needs and understanding your process and products, we develop solutions that make a real difference.

Additive 
  • Heat Stabilizer

Features 
  • Heat Stabilized

Processing Method 
  • Blow Molding

Resin ID (ISO 1043)
  • ISO 18064 TPC-ET

Physical
Nominal Value
Unit
Test Method
Density
1.15
g/cm³
ISO 1183
Melt Volume-Flow Rate (MVR) (230°C/10.0 kg)
0.488
in³/10min
ISO 1133
Water Absorption


ISO 62
Saturation, 73°F
0.70
%

Equilibrium, 73°F, 50% RH
0.30
%

Hardness
Nominal Value
Unit
Test Method
Shore Hardness


ISO 868
Shore D, 3 sec
39


Shore D, 15 sec
39


Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
9720
psi
ISO 527-2
Tensile Stress



Break 2
4640
psi
ISO 527-2
Break
3120
psi
ISO 527-2
5.0% Strain 2
493
psi
ISO 527-2
10% Strain 2
827
psi
ISO 527-2
10% Strain 3
725
psi
ISO 527-2
10% Strain
870
psi
ISO 527-2
10% Strain, -40°F 3
1810
psi
ISO 527-2
10% Strain, 212°F 3
377
psi
ISO 527-2
50% Strain
  • 1600

  • 1600

psi
ISO 527-2
50% Strain 2
1230
psi
ISO 527-2
100% Strain 2
1310
psi
ISO 527-2
100% Strain
2020
psi
ISO 527-2
Tensile Strain


ISO 527-2
Break
> 50
%

Break 2
950
%

Nominal Tensile Strain at Break
300
%
ISO 527-2
Elastomers
Nominal Value
Unit
Test Method
Tear Strength


ISO 34-1
--
540
lbf/in

-- 4, 5
1500
lbf/in

Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength


ISO 179/1eA
-22°F
No Break


73°F
No Break


Notched Izod Impact Strength


ISO 180/1A
-4°F
No Break


73°F
No Break


Thermal
Nominal Value
Unit
Test Method
Melting Temperature 6
415
°F
ISO 11357-3
Effective Thermal Diffusivity
8.60E-8
m²/s

Fill Analysis
Nominal Value
Unit

Melt Density
1.01
g/cm³

Melt Thermal Conductivity
1.3
Btu·in/hr/ft²/°F

Specific Heat Capacity of Melt
0.531
Btu/lb/°F



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields