Products

Arnitel® EB463

Arnitel® EB463

Manufacturer: DSM
Produced At:
 Europe / China
Product Category: Thermoplastic Copolyester Elastomer
Product No: Arnitel EB463 
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized

Arnitel® EB463

Thermoplastic Copolyester Elastomer
Product Description:
Blow Molding Grade

Special Features:
  • Heat stabilized or stable to heat


Used In:
  • Boots and Bellows


Arnitel® is a high-performance ThermoPlastic Copolyester (TPC) that offers you a unique combination of flexibility, high temperature resistance and strength - plus excellent processing characteristics.
In industries ranging from automotive to E&E, Arnitel® is increasingly being as a lighter, smarter, greener alternative to conventional rubbers €" reducing environmental impact and ultimately, system costs.
The product is supported by an experienced and knowledgeable global team continuously working on new ideas and applications, as well as exploring new markets. By listening to your needs and understanding your process and products, we develop solutions that make a real difference.

Additive 
  • Heat Stabilizer

Features 
  • Heat Stabilized

Processing Method 
  • Blow Molding

Resin ID (ISO 1043)
  • ISO 18064 TPC-ET

Physical
Nominal Value
Unit
Test Method
Density
1.15
g/cm³
ISO 1183
Melt Volume-Flow Rate (MVR) (230°C/10.0 kg)
0.641
in³/10min
ISO 1133
Water Absorption


ISO 62
Saturation, 73°F
0.70
%

Equilibrium, 73°F, 50% RH
0.30
%

Hardness
Nominal Value
Unit
Test Method
Shore Hardness (Shore D, 3 sec)
38

ISO 868
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
9430
psi
ISO 527-2
Tensile Stress


ISO 527-2
Break 2
3480
psi

Break
2610
psi

5.0% Strain 2
493
psi

5.0% Strain
508
psi

10% Strain 2
798
psi

10% Strain 3
769
psi

10% Strain
870
psi

10% Strain, 212°F 3
406
psi

50% Strain 2
1200
psi

50% Strain
1670
psi

100% Strain 2
1290
psi

100% Strain
2180
psi

Tensile Strain 2 (Break)
810
%
ISO 527-2
Nominal Tensile Strain at Break
200
%
ISO 527-2
Elastomers
Nominal Value
Unit
Test Method
Tear Strength 4, 5
1300
lbf/in
ISO 34-1
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength


ISO 179/1eA
-22°F
No Break


73°F
No Break


Charpy Unnotched Impact Strength


ISO 179/1eU
-22°F
No Break


73°F
No Break


Notched Izod Impact Strength


ISO 180/1A
-4°F
No Break


73°F
No Break


Thermal
Nominal Value
Unit
Test Method
Melting Temperature 6
397
°F
ISO 11357-3


Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation
展开