Texin® 970 U
Thermoplastic Polyurethane Elastomer (Polyether)
Texin 970U resin is an aromatic polyether-based thermoplastic polyurethane with a Shore hardness of approximately 70D. It can be processed by injection molding, extrusion, or blow molding.
Additive | |
Features | |
Uses | |
Processing Method | |
Density / Specific Gravity |
|
|
|
-- | 1.18 |
| ASTM D792 |
-- | 1.18 | g/cm³ | ISO 1183 |
Molding Shrinkage |
|
|
|
Flow : 0.100 in | 8.0E-3 | in/in | ASTM D955 |
Across Flow : 0.100 in | 8.0E-3 | in/in | ASTM D955 |
Across Flow : 0.100 in | 0.80 | % | ISO 2577 |
Flow : 0.100 in | 0.80 | % | ISO 2577 |
Durometer Hardness (Shore D) | 70 |
| ASTM D2240, ISO 868 |
Flexural Modulus |
|
| ASTM D790, ISO 178 |
-22°F | 293000 | psi |
|
73°F | 78000 | psi |
|
158°F | 17000 | psi |
|
Taber Abrasion Resistance |
|
|
|
1000 Cycles, 1000 g, H-18 Wheel | 75.0 | mg | ASTM D1044 |
1000 Cycles, 1000 g, H-18 Wheel | 75.0 | mg | ISO 4649 |
Tensile Stress |
|
| ASTM D412, ISO 37 |
50% Strain | 3000 | psi |
|
100% Strain | 3700 | psi |
|
300% Strain | 5700 | psi |
|
Tensile Strength (Yield) | 6900 | psi | ASTM D412, ISO 37 |
Tensile Elongation (Break) | 320 | % | ASTM D412, ISO 37 |
Tear Strength |
|
|
|
-- 2 | 1100 | lbf/in | ASTM D624 |
-- | 1100 | lbf/in | ISO 34-1 |
Compression Set |
|
| ASTM D395B, ISO 815 |
73°F, 22 hr | 40 | % |
|
73°F, 22 hr 3 | 25 | % |
|
158°F, 22 hr | 75 | % |
|
158°F, 22 hr 3 | 45 | % |
|
212°F, 22 hr | 90 | % |
|
212°F, 22 hr 3 | 65 | % |
|
Bayshore Resilience | 50 | % | ASTM D2632 |