Texin® 270
Thermoplastic Polyurethane Elastomer (Polyester)
Texin 270 resin is an aromatic polyester-based thermoplastic polyurethane with a Shore hardness of approximately 70D. It can be processed by injection molding; extrusion processes are not recommended.
Features   | - Fuel Resistant,Good Tear Strength,High Stiffness,Oil Resistant 
 
  | 
Uses   | - Gears,Sporting Goods,Wheels
 
  | 
Agency Ratings   | - FDA 21 CFR 177.1680,FDA 21 CFR 177.2600 
 
  | 
Appearance   |  | 
Processing Method   |  | 
Density / Specific Gravity  | 
  | 
  | 
  | 
--  | 1.24  | 
  | ASTM D792 | 
--  | 1.24  | g/cm³  | ISO 1183 | 
Molding Shrinkage  | 
  | 
  | 
  | 
Flow : 0.100 in  | 8.0E-3  | in/in  | ASTM D955 | 
Across Flow : 0.100 in  | 8.0E-3  | in/in  | ASTM D955 | 
Across Flow : 0.100 in  | 0.80  | %  | ISO 2577 | 
Flow : 0.100 in  | 0.80  | %  | ISO 2577 | 
Durometer Hardness (Shore D)  | 70  | 
  | ASTM D2240, ISO 868 | 
Flexural Modulus  | 
  | 
  | ASTM D790, ISO 178 | 
-22°F  | 422000  | psi  | 
  | 
73°F  | 105000  | psi  | 
  | 
158°F  | 14900  | psi  | 
  | 
Taber Abrasion Resistance  | 
  | 
  | 
  | 
1000 Cycles, 1000 g, H-18 Wheel  | 90.0  | mg  | ASTM D1044 | 
1000 Cycles, 1000 g, H-18 Wheel  | 90.0  | mg  | ISO 4649 | 
Tensile Stress  | 
  | 
  | ASTM D412, ISO 37 | 
50% Strain  | 4100  | psi  | 
  | 
100% Strain  | 4210  | psi  | 
  | 
300% Strain  | 6210  | psi  | 
  | 
Tensile Strength (Yield)  | 8210  | psi  | ASTM D412, ISO 37 | 
Tensile Elongation (Break)  | 400  | %  | ASTM D412, ISO 37 | 
Tear Strength  | 
  | 
  | 
  | 
-- 2  | 1300  | lbf/in  | ASTM D624 | 
--  | 1300  | lbf/in  | ISO 34-1 | 
Compression Set  | 
  | 
  | ASTM D395B, ISO 815 | 
73°F, 22 hr  | 50  | %  | 
  | 
73°F, 22 hr 3  | 30  | %  | 
  | 
158°F, 22 hr  | 85  | %  | 
  | 
158°F, 22 hr 3  | 45  | %  | 
  | 
Bayshore Resilience  | 55  | %  | ASTM D2632 |