Desmopan® 9370AU
Thermoplastic Polyurethane Elastomer (Polyether)
Extrusion- and injection molding grade; with special UV stabilizers; very good hydrolysis and microbial resistance; good low-temperature flexibility; free from plasticizers; high moisture vapor transmission rate; Application; breathable films; Films; Sports shoe soles; hard - soft systems
Additive | |
Features | |
Uses | - Film,Footwear,Sporting Goods
|
RoHS Compliance | |
Processing Method | - Extrusion,Injection Molding
|
Density |
|
|
|
73°F | 1.06 | g/cm³ | ISO 1183 |
-- | 0.0383 | lb/in³ | ISO 1183 3 |
Shore Hardness |
|
|
|
Shore A, 1 sec, 73°F | 70 |
| ISO 7619 |
Shore A, 3 sec | 70 |
| ISO 868 3 |
Tensile Stress 4 |
|
| DIN 53504 |
Break, 73°F | 3890 | psi |
|
100% Strain, 73°F | 421 | psi |
|
300% Strain, 73°F | 798 | psi |
|
Tensile Strain 4 (Break, 73°F) | 790 | % | DIN 53504 |
Abrasion Resistance 5 | 69.0 | mm³ | ISO 4649 |
Tensile Storage Modulus |
|
| ISO 6721 |
-4°F | 18130 | psi |
|
68°F | 1595 | psi |
|
140°F | 1305 | psi |
|
Tear Strength 6 (73°F) | 220 | lbf/in | ISO 34-1 |
Compression Set |
|
| ISO 815 |
73°F, 72 hr | 22 | % |
|
158°F, 24 hr 5 | 45 | % |
|
158°F, 24 hr 7 | 36 | % |
|
Rebound Resilience | 63 | % | ISO 4662 |
Drying Temperature | < 176 | °F |
|
Processing (Melt) Temp | 374 to 410 | °F |
|
Mold Temperature | 68 to 104 | °F |
|
Drying Temperature | < 176 | °F |
|