Desmopan® 89785A
Thermoplastic Polyurethane Elastomer
Grade for calandering; no yellowing under the action of UV light; very good low-temperature impact strength; high rebound resilience; improved microbial resistance; Improved hydrolysis resistance; Textile coating
Features | - Hydrolysis Resistant,Low Temperature Impact Resistance,Microbe Resistant,Resilient
|
Uses | - Coating Applications,Fabric Coatings
|
RoHS Compliance | |
Processing Method | |
Density (73°F) | 1.08 | g/cm³ | ISO 1183 |
Shore Hardness (Shore A, 1 sec, 73°F) | 86 |
| ISO 7619 |
Abrasion Resistance 2 | 30.0 | mm³ | ISO 4649 |
Tear Strength 3 (73°F) | 430 | lbf/in | ISO 34-1 |
Compression Set |
|
| ISO 815 |
73°F, 72 hr | 20 | % |
|
158°F, 24 hr 2 | 40 | % |
|
Rebound Resilience | 65 | % | ISO 4662 |
Processing (Melt) Temp | 392 to 428 | °F |
|
Mold Temperature | 68 to 104 | °F |
|
Melt Temperature | 374 | °F |
|