Desmopan® 588 L
Thermoplastic Polyurethane Elastomer
Extrusion- and injection molding grade; improved microbial resistance; Improved hydrolysis resistance; Application; Cable sheathings; Hoses, non-reinforced; Roof lining
Features | - Hydrolysis Resistant,Microbe Resistant
|
Uses | - Hose,Liners,Wire & Cable Applications
|
RoHS Compliance | |
Processing Method | - Extrusion,Injection Molding
|
Density (73°F) | 1.15 | g/cm³ | ISO 1183 |
Shore Hardness |
|
| ISO 7619 |
Shore A, 1 sec, 73°F | 88 |
|
|
Shore D, 1 sec, 73°F | 33 |
|
|
Tensile Stress 2 |
|
| DIN 53504 |
Break, 73°F | 5080 | psi |
|
10% Strain, 73°F | 290 | psi |
|
50% Strain, 73°F | 725 | psi |
|
100% Strain, 73°F | 870 | psi |
|
300% Strain, 73°F | 1600 | psi |
|
Tensile Strain 2 (Break, 73°F) | 700 | % | DIN 53504 |
Abrasion Resistance 3 | 60.0 | mm³ | ISO 4649 |
Tensile Storage Modulus |
|
| ISO 6721 |
-4°F | 23931 | psi |
|
68°F | 4206 | psi |
|
140°F | 2901 | psi |
|
Tear Strength 4 (73°F) | 310 | lbf/in | ISO 34-1 |
Compression Set |
|
| ISO 815 |
73°F, 72 hr | 25 | % |
|
158°F, 24 hr 3 | 35 | % |
|
158°F, 24 hr 5 | 26 | % |
|
Rebound Resilience | 36 | % | ISO 4662 |
Drying Temperature | < 176 | °F |
|
Processing (Melt) Temp | 410 to 446 | °F |
|
Mold Temperature | 68 to 104 | °F |
|
Drying Temperature | < 176 | °F |
|
Melt Temperature | 374 to 410 | °F |
|