Desmopan® 392
Thermoplastic Polyurethane Elastomer
Extrusion- and injection molding grade; high mechanical strength; Application; Toothed belts; Profiles; Hoses, non-reinforced
Features | |
Uses | |
RoHS Compliance | |
Processing Method | - Extrusion,Injection Molding
|
Density (73°F) | 1.21 | g/cm³ | ISO 1183 |
Shore Hardness |
|
| ISO 7619 |
Shore A, 1 sec, 73°F | 92 |
|
|
Shore D, 1 sec, 73°F | 40 |
|
|
Tensile Stress 2 |
|
| DIN 53504 |
Break, 73°F | 7400 | psi |
|
10% Strain, 73°F | 609 | psi |
|
50% Strain, 73°F | 1130 | psi |
|
100% Strain, 73°F | 1330 | psi |
|
300% Strain, 73°F | 3050 | psi |
|
Tensile Strain 2 (Break, 73°F) | 560 | % | DIN 53504 |
Abrasion Resistance 3 | 25.0 | mm³ | ISO 4649 |
Tensile Storage Modulus |
|
| ISO 6721 |
-4°F | 65992 | psi |
|
68°F | 13053 | psi |
|
140°F | 8557 | psi |
|
Tear Strength 4 (73°F) | 460 | lbf/in | ISO 34-1 |
Compression Set |
|
| ISO 815 |
73°F, 72 hr | 25 | % |
|
158°F, 24 hr 3 | 36 | % |
|
158°F, 24 hr 5 | 25 | % |
|
Rebound Resilience | 33 | % | ISO 4662 |
Drying Temperature | < 176 | °F |
|
Processing (Melt) Temp | 410 to 446 | °F |
|
Mold Temperature | 68 to 104 | °F |
|
Drying Temperature | < 176 | °F |
|