VESTAMID® L LX9009
Polyamide 12
Unfilled VESTAMID® polyamide 12 compounds
Characterization: medium viscosity, light stabilized
Applications: ski cover films
In general, it can be said that long-chain, semi-crystalline polyamides absorb little water, are resistant to polar and non-polar solvents, exhibit low creep behavior and high impact resistance and can be used in a wide temperature range. Virtually no other polymer material in this price range exhibits these properties.
Additive | - Heat Stabilizer,UV Stabilizer
|
Features | - Abrasion Resistant,Excellent Processability,Fatigue Resistant,Food Contact Acceptable,Fuel Resistant,Grease Resistant,Heat Stabilized,High ESCR (Stress Crack Resist.),High Impact Resistance,Light Stabilized,Low Friction,Low Temperature Impact Resistance,Low to No Water Absorption,Medium Viscosity,Noise Damping,Oil Resistant,Semi Crystalline,Solvent Resistant,Vibration Damping
|
Uses | |
Agency Ratings | - EU 10/2011,FDA 21 CFR 177.1500
|
Appearance | - Colors Available,Natural Color
|
Forms | |
Processing Method | |
Tensile Modulus | 189000 | psi | ISO 527-2 |
Tensile Stress |
|
| ISO 527-2 |
Yield | 5950 | psi |
|
Break | 8410 | psi |
|
Tensile Strain |
|
| ISO 527-2 |
Yield | 5.0 | % |
|
Break | > 50 | % |
|
Charpy Notched Impact Strength |
|
| ISO 179/1eA |
-22°F, Complete Break | 3.3 | ft·lb/in² |
|
73°F, Complete Break | 4.8 | ft·lb/in² |
|
Charpy Unnotched Impact Strength |
|
| ISO 179/1eU |
-22°F | No Break |
|
|
73°F | No Break |
|
|
Heat Deflection Temperature |
|
|
|
66 psi, Unannealed | 264 | °F | ISO 75-2/B |
264 psi, Unannealed | 124 | °F | ISO 75-2/A |
Vicat Softening Temperature |
|
|
|
-- | 338 | °F | ISO 306/A |
-- | 284 | °F | ISO 306/B |
Melting Temperature 2 | 352 | °F | ISO 11357-3 |
ISO Shortname | PA12, FL, 16-010 |
| ISO 1874 |