15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance

Filler / Reinforcement 
  • Glass Fiber, 15% Filler by Weight

Features 
  • Good Impact Resistance

RoHS Compliance 
  • Contact Manufacturer

Processing Method 
  • Injection Molding

Part Marking Code (ISO 11469)
  • PET-IGF15

Resin ID (ISO 1043)
  • PET-IGF15

Physical
Nominal Value
Unit
Test Method
Density
1.39
g/cm³
ISO 1183
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
653000
psi
ISO 527-2
Tensile Stress (Break)
11600
psi
ISO 527-2
Tensile Strain (Break)
5.0
%
ISO 527-2
Flexural Modulus
580000
psi
ISO 178
Poisson's Ratio
0.36

ISO 527
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength (73°F)
5.2
ft·lb/in²
ISO 179/1eA
Charpy Unnotched Impact Strength (73°F)
26
ft·lb/in²
ISO 179/1eU
Notched Izod Impact Strength (73°F)
5.2
ft·lb/in²
ISO 180/1A
Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
374
°F
ISO 75-2/A
Melting Temperature 3
482
°F
ISO 11357-3
Electrical
Nominal Value
Unit
Test Method
Surface Resistivity
1.0E+14
ohms
IEC 60093
Volume Resistivity
1.0E+14
ohms·cm
IEC 60093
Electric Strength
860
V/mil
IEC 60243-1
Relative Permittivity


IEC 60250
100 Hz
4.40


1 MHz
3.90


Dissipation Factor


IEC 60250
100 Hz
0.042


1 MHz
0.023


Comparative Tracking Index
350
V
IEC 60112
Flammability
Nominal Value
Unit
Test Method
Burning Rate 4 (0.0394 in)
< 3.9
in/min
ISO 3795
Flame Rating


UL 94, IEC 60695-11-10, -20
0.030 in
HB


0.06 in
HB


FMVSS Flammability
B

FMVSS 302
Fill Analysis
Nominal Value
Unit

Ejection Temperature
338
°F

Injection
Nominal Value
Unit

Drying Temperature
248
°F

Drying Time - Desiccant Dryer
4.0 to 6.0
hr

Suggested Max Moisture
0.020
%

Processing (Melt) Temp
518 to 554
°F

Melt Temperature, Optimum
545
°F

Mold Temperature
167 to 203
°F

Mold Temperature, Optimum
203
°F

Holding Pressure
11600
psi

Back Pressure
As low as possible


Drying Recommended
yes


Hold Pressure Time
4.00
s/mm

Maximum Screw Tangential Speed
472
in/min