Crastin® S650FR NC010

Crastin® S650FR NC010

Manufacturer: DUPONT
Produced At:
 Import/ China
Product Category: PBT
Product No:
 Crastin S650FR NC010
Product Quantity: 25KG / BAG
Product Features:
 Flame Retardant

Crastin® S650FR NC010

THERMOPLASTIC POLYESTER RESIN
Product Description:
Unreinforced, Flame Retardant, Polybutylene Terephthalate

Additive 
  • Flame Retardant

Features 
  • Flame Retardant

RoHS Compliance 
  • Contact Manufacturer

Forms 
  • Pellets

Processing Method 
  • Injection Molding

Part Marking Code (ISO 11469)
  • PBT-FR(17)

Resin ID (ISO 1043)
  • PBT-FR(17)

Physical
Nominal Value
Unit
Test Method
Density
1.46
g/cm³
ISO 1183
Molding Shrinkage


ISO 294-4
Across Flow
1.6
%

Across Flow  3
2.2
%

Flow
1.8
%

Flow  3
2.2
%

Water Absorption


ISO 62
Saturation, 73°F, 0.0787 in
0.39
%

Equilibrium, 73°F, 0.0787 in, 50% RH
0.15
%

Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
435000
psi
ISO 527-2
Tensile Stress (Yield)
9430
psi
ISO 527-2
Tensile Strain (Yield)
4.6
%
ISO 527-2
Nominal Tensile Strain at Break
7.2
%
ISO 527-2
Tensile Creep Modulus


ISO 899-1
1 hr
363000
psi

1000 hr
261000
psi

Flexural Stress
14500
psi
ISO 178
Poisson's Ratio
0.37

ISO 527
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength


ISO 179/1eA
-22°F
1.7
ft·lb/in²

73°F
1.9
ft·lb/in²

Charpy Unnotched Impact Strength


ISO 179/1eU
-22°F
31
ft·lb/in²

73°F
33
ft·lb/in²

Notched Izod Impact Strength


ISO 180/1A
-22°F
1.9
ft·lb/in²

73°F
1.9
ft·lb/in²

Unnotched Izod Impact Strength


ISO 180/1U
-22°F
20
ft·lb/in²

73°F
21
ft·lb/in²

Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature



66 psi, Unannealed
320
°F
ISO 75-2/B
264 psi, Unannealed
149
°F
ISO 75-2/A
Vicat Softening Temperature
347
°F
ISO 306/B50
Melting Temperature 4
430
°F
ISO 11357-3
CLTE


ISO 11359-2
Flow
6.7E-5
in/in/°F

Transverse
6.7E-5
in/in/°F

Electrical
Nominal Value
Unit
Test Method
Surface Resistivity
1.0E+15
ohms
IEC 60093
Volume Resistivity
> 1.0E+15
ohms·cm
IEC 60093
Electric Strength
640
V/mil
IEC 60243-1
Relative Permittivity


IEC 60250
100 Hz
3.40


1 MHz
3.50


Dissipation Factor


IEC 60250
100 Hz
7.1E-4


1 MHz
0.018


Comparative Tracking Index
225
V
IEC 60112
Flammability
Nominal Value
Unit
Test Method
Flame Rating


UL 94, IEC 60695-11-10, -20
0.030 in
V-0


0.06 in
V-0


Oxygen Index
30
%
ISO 4589-2
FMVSS Flammability
DNI

FMVSS 302
Fill Analysis
Nominal Value
Unit

Ejection Temperature
338
°F

Injection
Nominal Value
Unit

Drying Temperature
248
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Suggested Max Moisture
0.040
%

Processing (Melt) Temp
464 to 500
°F

Melt Temperature, Optimum
482
°F

Mold Temperature
86 to 266
°F

Mold Temperature, Optimum
176
°F

Holding Pressure
8700
psi

Back Pressure
As low as possible


Drying Recommended
yes


Hold Pressure Time
3.00
s/mm



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields