Radilon® S 40EPT2808 333 NER
Polyamide 6
PA6 high viscosity extrusion grade. Low modulus, high flexibility and high impact strength, even at low temperatures. Black colour.
This material has been designed for extrusion of pipes. Typical application: convoluted fuel pipes for the automotive industry.
Features | |
Uses | - Automotive Applications,Piping
|
RoHS Compliance | |
Appearance | |
Processing Method | |
Resin ID (ISO 1043) | |
Density | 1.08 | -- | g/cm³ | ISO 1183 |
Tensile Modulus | 131000 | -- | psi | ISO 527-2/1A/1 |
Tensile Stress (Yield) | 5080 | -- | psi | ISO 527-2/1A/50 |
Nominal Tensile Strain at Break | > 100 | -- | % | ISO 527-2/1A/50 |
Flexural Modulus 2 | 79800 | -- | psi | ISO 178 |
Flexural Stress 2 | 3630 | -- | psi | ISO 178 |
Charpy Notched Impact Strength(73°F) | 31 | -- | ft·lb/in² | ISO 179/1eA |
Heat Deflection Temperature (264 psi, Unannealed) | 122 | -- | °F | ISO 75-2/Af |
Vicat Softening Temperature | 248 | -- | °F | ISO 306/B50 |
Melting Temperature 3 | 428 | -- | °F | ISO 11357-3 |
Surface Resistivity 4 | 1.0E+12 | 1.0E+10 | ohms | IEC 60093 |
Volume Resistivity 4 | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
Comparative Tracking Index(Solution A) | 600 | -- | V | IEC 60112 |
Flame Rating (0.031 in) | HB | -- |
| UL 94 |
Flammability | < 1 | -- | in/min | FMVSS 302 |
Drying Temperature - Desiccant Dryer | 176 | °F |
|
Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr |
|
Dew Point - Desiccant Dryer | -4 | °F |
|
Suggested Max Moisture | 0.15 | % |
|
Processing (Melt) Temp | 482 to 536 | °F |
|
Mold Temperature | 158 to 176 | °F |
|
Injection Rate | Moderate |
|
|
Melt Temperature | 464 to 518 | °F |
|