Radilon® A RV500RW 182 NAT 5346
Polyamide 66
PA66 50% glass fiber reinforced injection moulding grade. Heat stabilized. Natural colour.
Suitable for technical parts requiring very high stiffness and high mechanical resistance. Excellent heat ageing properties retention, improved welding lines strength. Especially fit for demanding metal replacement applications.
Filler / Reinforcement | |
Additive | |
Features | - Heat Aging Resistant,Heat Stabilized,High Stiffness
|
Uses | |
RoHS Compliance | |
Appearance | |
Processing Method | |
Resin ID (ISO 1043) | |
Density | 1.58 | -- | g/cm³ | ISO 1183 |
Water Absorption |
|
|
| ISO 62 |
Saturation, 73°F, 0.0787 in | 4.0 | -- | % |
|
Equilibrium, 73°F, 0.0787 in, 50% RH | 1.1 | -- | % |
|
Tensile Modulus | 2.54E+6 | -- | psi | ISO 527-2/1A/1 |
Tensile Stress (Break) | 35500 | -- | psi | ISO 527-2/1A/5 |
Tensile Strain (Break) | 2.9 | -- | % | ISO 527-2/1A/5 |
Flexural Modulus 2 | 2.32E+6 | -- | psi | ISO 178 |
Flexural Stress 2 | 290 | -- | psi | ISO 178 |
Charpy Unnotched Impact Strength |
|
|
| ISO 179/1eU |
-22°F | 45 | -- | ft·lb/in² |
|
73°F | 180 | -- | ft·lb/in² |
|
Heat Deflection Temperature |
|
|
|
|
66 psi, Unannealed | 419 | -- | °F | ISO 75-2/Bf |
264 psi, Unannealed | 491 | -- | °F | ISO 75-2/Af |
Vicat Softening Temperature | 491 | -- | °F | ISO 306/B50 |
Melting Temperature 3 | 500 | -- | °F | ISO 11357-3 |
Surface Resistivity 4 | 1.0E+12 | 1.0E+10 | ohms | IEC 60093 |
Volume Resistivity 4 | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
Flame Rating (0.031 in) | HB | -- |
| UL 94 |
Flammability | 0 | -- | in/min | FMVSS 302 |
Drying Temperature - Desiccant Dryer | 176 | °F |
|
Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr |
|
Dew Point - Desiccant Dryer | -4 | °F |
|
Suggested Max Moisture | 0.15 | % |
|
Processing (Melt) Temp | 536 to 572 | °F |
|
Mold Temperature | 176 to 212 | °F |
|
Injection Rate | Fast |
|
|