Radilon® A RV300RG 3900 NER 8468
Polyamide 66
PA66 30% glass fiber reinforced injection moulding grade. Heat stabilized, high hydrolysis resistance. Deep black colour.
Suitable for parts requiring high stiffness and good mechanical resistance. Particularly fit to work in contact with automotive cooling circuit liquids.
Filler / Reinforcement | |
Additive | |
Features | - Heat Stabilized,High Stiffness,Hydrolysis Resistant
|
Uses | |
RoHS Compliance | |
Appearance | |
Processing Method | |
Resin ID (ISO 1043) | |
Density | 1.37 | -- | g/cm³ | ISO 1183 |
Water Absorption |
|
|
| ISO 62 |
Saturation, 73°F, 0.0787 in | 7.0 | -- | % |
|
Equilibrium, 73°F, 0.0787 in, 50% RH | 1.7 | -- | % |
|
Tensile Modulus | 1.45E+6 | -- | psi | ISO 527-2/1A/1 |
Tensile Stress (Break) | 29000 | -- | psi | ISO 527-2/1A/5 |
Tensile Strain (Break) | 3.6 | -- | % | ISO 527-2/1A/5 |
Flexural Modulus 2 | 1.41E+6 | -- | psi | ISO 178 |
Flexural Stress 2 | 45000 | -- | psi | ISO 178 |
Charpy Notched Impact Strength(73°F) | 6.7 | -- | ft·lb/in² | ISO 179/1eA |
Charpy Unnotched Impact Strength(73°F) | 43 | -- | ft·lb/in² | ISO 179/1eU |
Heat Deflection Temperature (264 psi, Unannealed) | 464 | -- | °F | ISO 75-2/Af |
Vicat Softening Temperature | 482 | -- | °F | ISO 306/B50 |
Melting Temperature 3 | 500 | -- | °F | ISO 11357-3 |
Surface Resistivity 4 | 1.0E+12 | 1.0E+10 | ohms | IEC 60093 |
Volume Resistivity 4 | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
Burning Rate (0.118 in) | 0.0 | -- | in/min | ISO 3795 |
Flame Rating (0.031 in) | HB | -- |
| UL 94 |
Glow Wire Flammability Index (0.08 in) | 1290 | -- | °F | IEC 60695-2-12 |
Drying Temperature - Desiccant Dryer | 176 | °F |
|
Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr |
|
Dew Point - Desiccant Dryer | -4 | °F |
|
Suggested Max Moisture | 0.15 | % |
|
Processing (Melt) Temp | 536 to 572 | °F |
|
Mold Temperature | 176 to 212 | °F |
|
Injection Rate | Moderate-Fast |
|
|