Radilon® A CP300K 333 NER
Polyamide 66
PA66 30% mineral filled injection moulding grade. Heat stabilized. Black colour.
Suitable for parts requiring good dimensional stability, reduced shrinkage and low warpage.
ISO 1043 : PA66-T MX30
Filler / Reinforcement   |  | 
Additive   |  | 
Features   | - Good Dimensional Stability,Heat Stabilized,Low Shrinkage
 
  | 
RoHS Compliance   |  | 
Appearance   |  | 
Processing Method   |  | 
Resin ID (ISO 1043)  |  | 
Density  | 1.36  | --  | g/cm³  | ISO 1183 | 
Molding Shrinkage 2  | 
  | 
  | 
  | ISO 294-4 | 
Across Flow  | 1.5  | --  | %  | 
  | 
Flow  | 1.4  | --  | %  | 
  | 
Water Absorption  | 
  | 
  | 
  | ISO 62 | 
Saturation, 73°F, 0.0787 in  | 6.1  | --  | %  | 
  | 
Equilibrium, 73°F, 0.0787 in, 50% RH  | 1.9  | --  | %  | 
  | 
Tensile Modulus  | 754000  | 609000  | psi  | ISO 527-2/1A/1 | 
Tensile Stress (Break)  | 13100  | 9430  | psi  | ISO 527-2/1A/5 | 
Tensile Strain (Break)  | 8.0  | 12  | %  | ISO 527-2/1A/5 | 
Flexural Modulus 3  | 653000  | --  | psi  | ISO 178 | 
Flexural Stress 3  | 19600  | --  | psi  | ISO 178 | 
Charpy Notched Impact Strength  | 
  | 
  | 
  | ISO 179/1eA | 
-22°F  | 1.9  | --  | ft·lb/in²  | 
  | 
73°F  | 2.1  | 2.4  | ft·lb/in²  | 
  | 
Charpy Unnotched Impact Strength  | 
  | 
  | 
  | ISO 179/1eU | 
-22°F  | 19  | --  | ft·lb/in²  | 
  | 
73°F  | 26  | 33  | ft·lb/in²  | 
  | 
Heat Deflection Temperature  | 
  | 
  | 
  | 
  | 
66 psi, Unannealed  | 419  | --  | °F  | ISO 75-2/Bf | 
264 psi, Unannealed  | 194  | --  | °F  | ISO 75-2/Af | 
Vicat Softening Temperature  | 473  | --  | °F  | ISO 306/B50 | 
Melting Temperature  | 500  | --  | °F  | ISO 11357 | 
Surface Resistivity  | 1.0E+12  | 1.0E+10  | ohms  | IEC 60093 | 
Volume Resistivity  | 1.0E+15  | 1.0E+13  | ohms·cm  | IEC 60093 | 
Comparative Tracking Index  | 500  | --  | V  | IEC 60112 | 
Burning Rate  | 0.0  | --  | in/min  | FMVSS 302 | 
Flame Rating (0.031 in)  | HB  | --  | 
  | UL 94 | 
Glow Wire Flammability Index (0.08 in)  | 1290  | --  | °F  | IEC 60695-2-12 | 
Drying Temperature - Desiccant Dryer  | 176  | °F  | 
  | 
Drying Time - Desiccant Dryer  | 2.0 to 4.0  | hr  | 
  | 
Dew Point - Desiccant Dryer  | < -4  | °F  | 
  | 
Suggested Max Moisture  | 0.15  | %  | 
  | 
Processing (Melt) Temp  | 536 to 572  | °F  | 
  | 
Mold Temperature  | 176 to 212  | °F  | 
  | 
Injection Rate  | Moderate-Fast  | 
  | 
  |