Radilon® D E50ZW 333 NER 6463
Polyamide 610
PA610 flexible extrusion grade. Toughened and heat stabilized. Good resistance to Zinc Chloride solution. Black colour.
Suitable for extrusion of pipes, profiles and cable jackets.
This grade is partially renewably-sourced (60% of base polymer by weight).
Additive | |
Features | - Heat Stabilized,Renewable Resource Content
|
Uses | - Jacketing,Piping,Wire & Cable Applications
|
RoHS Compliance | |
Appearance | |
Processing Method | - Extrusion,Pipe Extrusion,Profile Extrusion
|
Resin ID (ISO 1043) | |
Density | 1.01 | -- | g/cm³ | ISO 1183 |
Water Absorption |
|
|
| ISO 62 |
Saturation, 73°F, 0.0787 in | 2.2 | -- | % |
|
Equilibrium, 73°F, 0.0787 in, 50% RH | 0.90 | -- | % |
|
Tensile Modulus | 160000 | 102000 | psi | ISO 527-2/1A/1 |
Tensile Stress (Yield) | 4350 | 3340 | psi | ISO 527-2/1A/50 |
Tensile Strain (Yield) | 7.5 | > 50 | % | ISO 527-2/1A/50 |
Nominal Tensile Strain at Break | > 50 | > 100 | % | ISO 527-2/1A/50 |
Flexural Modulus 2 | 138000 | -- | psi | ISO 178 |
Flexural Stress 2 | 4350 | -- | psi | ISO 178 |
Charpy Notched Impact Strength(73°F) | 36 | 40 | ft·lb/in² | ISO 179/1eA |
Heat Deflection Temperature (264 psi, Unannealed) | 122 | -- | °F | ISO 75-2/Af |
Vicat Softening Temperature | 257 | -- | °F | ISO 306/B50 |
Melting Temperature 3 | 428 | -- | °F | ISO 11357-3 |
Drying Temperature - Desiccant Dryer | 176 | °F |
|
Drying Time - Desiccant Dryer | 2.0 to 4.0 | hr |
|
Dew Point - Desiccant Dryer | -4 | °F |
|
Suggested Max Moisture | 0.10 | % |
|
Processing (Melt) Temp | 446 to 500 | °F |
|
Mold Temperature | 158 to 176 | °F |
|
Injection Rate | Moderate |
|
|
Melt Temperature | 446 to 482 | °F |
|