Products

Heramid® S NER GFP 3010

Heramid® S NER GFP 3010

Manufacturer: RADICI
Produced At:
 Europe / China
Product Category: Polyamide 66 (Nylon 6)
Product No: Heramid S NER GFP 3010 
Product Quantity: 25KG / BAG
Product Features: 
Glass\Mineral, 30% Filler by Weight

Heramid® S NER GFP 3010

Polyamide 6
Product Description:

PA6 30% glass fiber and mineral filler reinforced injection moulding grade. Black colour.

Post-industrial grade produced with selected polymers coming from polymerization, fibres and compounding plants.

ISO 1043 : PA6 (GF+MX)30


Filler / Reinforcement 
  • Glass\Mineral, 30% Filler by Weight

Recycled Content 
  • Yes

RoHS Compliance 
  • RoHS Compliant

Appearance 
  • Black

Processing Method 
  • Injection Molding

Resin ID (ISO 1043)
  • PA6 (GF+MX)30

Physical
Nominal Value
Unit
Test Method
Density
1.34
g/cm³
ISO 1183
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
943000
psi
ISO 527-2/1A/1
Tensile Stress (Break)
12300
psi
ISO 527-2/1A/5
Tensile Strain (Break)
2.0
%
ISO 527-2/1A/5
Flexural Modulus 2
928000
psi
ISO 178
Flexural Stress 2
19600
psi
ISO 178
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength (73°F)
2.9
ft·lb/in²
ISO 179/1eA
Charpy Unnotched Impact Strength (73°F)
17
ft·lb/in²
ISO 179/1eU
Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
374
°F
ISO 75-2/Af
Melting Temperature 3
432
°F
ISO 11357
Flammability
Nominal Value

Test Method
Flame Rating (0.031 in)
HB

UL 94
Injection
Nominal Value
Unit

Drying Temperature - Desiccant Dryer
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Dew Point - Desiccant Dryer
< -4
°F

Suggested Max Moisture
0.15
%

Processing (Melt) Temp
464 to 536
°F

Mold Temperature
176 to 194
°F

Injection Rate
Moderate-Fast




Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation