Stanyl® TS200B3

Stanyl® TS200B3

Manufacturer: DSM
Produced At:
 Europe / China
Product Category: Polyamide 46
PA46
Product No: Stanyl TS200B3
Product Quantity: 25KG / BAG
Product Features: Lubricated、15%CF

Stanyl® TS200B3

Polyamide 46
Product Description:
15% Carbon Reinforced

Special Features:
  • Lubricated


Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.

Filler / Reinforcement 
  • Carbon Fiber, 15% Filler by Weight

Additive 
  • Lubricant

Features 
  • Lubricated

Processing Method 
  • Injection Molding

Resin ID (ISO 1043)
  • PA46-CF15

Physical
Dry
Conditioned
Unit
Test Method
Density
1.22
--
g/cm³
ISO 1183
Water Absorption



ISO 62
Saturation, 73°F
12
--
%

Equilibrium, 73°F, 50% RH
3.2
--
%

Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
1.89E+6
--
psi
ISO 527-2
Tensile Stress (Break)
26800
16000
psi
ISO 527-2
Tensile Strain (Break)
2.0
4.0
%
ISO 527-2
Flexural Modulus
1.52E+6
841000
psi
ISO 178
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength(73°F)
2.4
--
ft·lb/in²
ISO 179/1eA
Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
554
--
°F
ISO 75-2/A
Glass Transition Temperature 3
167
--
°F
ISO 11357-2
Melting Temperature 3
563
--
°F
ISO 11357-3
CLTE



ISO 11359-2
Flow
1.4E-5
--
in/in/°F

Transverse
2.8E-5
--
in/in/°F


Injection
Dry
Unit
Drying Temperature
176
°F
Drying Time
4.0 to 8.0
hr
Rear Temperature
536 to 608
°F
Middle Temperature
572 to 608
°F
Front Temperature
572 to 608
°F
Nozzle Temperature
572 to 608
°F
Processing (Melt) Temp
581 to 608
°F
Mold Temperature
176 to 248
°F
Injection Rate
Moderate-Fast

Back Pressure
290 to 1450
psi
Screw Compression Ratio
2.5:1.0



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields