Products

Stanyl® TQ300F5

Stanyl® TQ300F5

Manufacturer: DSM
Produced At:
 Europe / China
Product Category: Polyamide 46
PA46
Product No: Stanyl TQ300F5
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized

Stanyl® TQ300F5

Polyamide 46
Product Description:
25% Glass Reinforced, Heat Stabilized

Special Features:
  • Heat stabilized or stable to heat


Used In:
  • Automotive Bearing Cages


Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.

Filler / Reinforcement 
  • Glass Fiber, 25% Filler by Weight

Additive 
  • Heat Stabilizer

Features 
  • Heat Stabilized

Uses 
  • Automotive Applications、Bearings 
Processing Method 
  • Injection Molding

Resin ID (ISO 1043)
  • PA46-GF25

Physical
Nominal Value
Unit
Test Method
Density
1.37
g/cm³
ISO 1183
Molding Shrinkage


ISO 294-4
Across Flow
1.4
%

Flow
0.50
%

Water Absorption


ISO 62
Saturation, 73°F
10
%

Equilibrium, 73°F, 50% RH
2.8
%

Viscosity Number
150
cm³/g
ISO 307
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
1.26E+6
psi
ISO 527-2
Tensile Stress (Break)
26800
psi
ISO 527-2
Tensile Strain (Break)
4.0
%
ISO 527-2
Impact
Nominal Value
Unit
Test Method
Notched Izod Impact Strength (73°F)
4.8
ft·lb/in²
ISO 180/1A
Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature



66 psi, Unannealed
554
°F
ISO 75-2/B
264 psi, Unannealed
554
°F
ISO 75-2/A
Glass Transition Temperature 2
167
°F
ISO 11357-2
Vicat Softening Temperature
554
°F
ISO 306/B50
Melting Temperature 2
563
°F
ISO 11357-3
CLTE


ISO 11359-2
Flow
1.4E-5
in/in/°F

Transverse
3.3E-5
in/in/°F

Electrical
Nominal Value
Unit
Test Method
Volume Resistivity
> 1.0E+15
ohms·cm
IEC 60093

Injection
Nominal Value
Unit
Drying Temperature
176
°F
Drying Time
2.0
hr
Rear Temperature
536 to 608
°F
Middle Temperature
572 to 608
°F
Front Temperature
572 to 608
°F
Nozzle Temperature
572 to 608
°F
Processing (Melt) Temp
581 to 608
°F
Mold Temperature
176 to 248
°F
Injection Rate
Moderate-Fast

Back Pressure
290 to 1450
psi
Screw Compression Ratio
2.5:1.0



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields