Products

Stanyl® TE373

Stanyl® TE373

Manufacturer: DSM
Produced At:
 Europe / China
Product Category: Polyamide 46
PA46
Product No: Stanyl TE373
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized

Stanyl® TE373

Polyamide 46
Product Description:
Heat Stabilized, Wear and Friction Modified

Special Features:
  • Heat stabilized or stable to heat

  • Wear and friction modified


Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.

Additive 
  • Heat Stabilizer

Features 
  • Heat Stabilized

Processing Method 
  • Injection Molding

Multi-Point Data 
  • Shear Modulus vs. Temperature (ISO 11403-1)

Resin ID (ISO 1043)
  • PA46

Physical
Dry
Conditioned
Unit
Test Method
Density
1.17
--
g/cm³
ISO 1183
Molding Shrinkage



ISO 294-4
Across Flow
2.0
--
%

Flow
2.0
--
%

Water Absorption



ISO 62
Saturation, 73°F
12
--
%

Equilibrium, 73°F, 50% RH
3.4
--
%

Viscosity Number
180
--
cm³/g
ISO 307
Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
406000
145000
psi
ISO 527-2
Tensile Stress (Yield)
12300
7250
psi
ISO 527-2
Tensile Strain (Yield)
10
20
%
ISO 527-2
Nominal Tensile Strain at Break
10
15
%
ISO 527-2
Flexural Modulus
348000
--
psi
ISO 178
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-22°F
1.9
1.9
ft·lb/in²

73°F
2.4
4.8
ft·lb/in²

Charpy Unnotched Impact Strength



ISO 179/1eU
-22°F
50
57
ft·lb/in²

73°F
71 ft·lb/in²
No Break


Notched Izod Impact Strength



ISO 180/1A
-40°F
1.9
1.9
ft·lb/in²

73°F
2.4
4.3
ft·lb/in²

Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
374
--
°F
ISO 75-2/A
Glass Transition Temperature 2
167
--
°F
ISO 11357-2
Melting Temperature 2
563
--
°F
ISO 11357-3
CLTE



ISO 11359-2
Flow
4.7E-5
--
in/in/°F

Transverse
6.1E-5
--
in/in/°F

Effective Thermal Diffusivity
8.96E-8
--
m²/s

Fill Analysis
Dry
Conditioned
Unit

Melt Density
1.00
--
g/cm³

Melt Thermal Conductivity
1.8
--
Btu·in/hr/ft²/°F

Specific Heat Capacity of Melt
0.664
--
Btu/lb/°F


Injection
Dry
Unit
Drying Temperature
176
°F
Drying Time
4.0 to 8.0
hr
Rear Temperature
536 to 608
°F
Middle Temperature
572 to 608
°F
Front Temperature
572 to 608
°F
Nozzle Temperature
572 to 608
°F
Processing (Melt) Temp
590 to 608
°F
Mold Temperature
176 to 248
°F
Injection Rate
Moderate-Fast

Back Pressure
290 to 1450
psi
Screw Compression Ratio
2.5:1.0



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields