Products

Stanyl® HGR1

Stanyl® HGR1

Manufacturer: DSM
Produced At:
 Europe / China
Product Category: Polyamide 46
PA46
Product No: Stanyl HGR1
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized

Stanyl® HGR1

Polyamide 46
Product Description:
Heat Stabilized, Wear and Friction Modified

Special Features:
  • Heat stabilized or stable to heat

  • Wear and friction modified


Used In:
  • Slide Shoe Surfaces in new generation

  • New Generation Slide Shoe Surfaces


Stanyl® is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.

Additive 
  • Heat Stabilizer

Features 
  • Heat Stabilized

Resin ID (ISO 1043)
  • PA46

Physical
Dry
Conditioned
Unit
Test Method
Density
1.18
--
g/cm³
ISO 1183
Molding Shrinkage



ISO 294-4
Across Flow
1.4
--
%

Flow
1.4
--
%

Water Absorption



ISO 62
Saturation, 73°F
13
--
%

Equilibrium, 73°F, 50% RH
3.2
--
%

Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus



ISO 527-2
--
537000
174000
psi

248°F
160000
--
psi

320°F
138000
--
psi

356°F
131000
--
psi

392°F
116000
--
psi

Tensile Stress



ISO 527-2
Yield, 248°F
7250
--
psi

Yield, 320°F
5800
--
psi

Yield, 356°F
5800
--
psi

Yield, 392°F
5080
--
psi

Break
14500
7980
psi

Nominal Tensile Strain at Break



ISO 527-2
--
6.0
30
%

356°F
> 50
--
%

392°F
> 50
--
%

Flexural Modulus



ISO 178
--
464000
145000
psi

248°F
160000
--
psi

320°F
123000
--
psi

Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-22°F
1.4
1.2
ft·lb/in²

73°F
2.4
7.1
ft·lb/in²

Thermal
Dry
Conditioned
Unit
Test Method
Melting Temperature 2
563
--
°F
ISO 11357-3
CLTE



ISO 11359-2
Flow
4.4E-5
--
in/in/°F

Transverse
3.9E-5
--
in/in/°F


Injection
Dry
Unit
Drying Temperature
176
°F
Drying Time
2.0
hr
Rear Temperature
536 to 608
°F
Middle Temperature
572 to 608
°F
Front Temperature
572 to 608
°F
Nozzle Temperature
572 to 608
°F
Processing (Melt) Temp
590 to 608
°F
Mold Temperature
176 to 248
°F
Injection Rate
Moderate-Fast

Back Pressure
290 to 1450
psi
Screw Compression Ratio
2.5:1.0



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields