Products

Terluran® HI-10

Terluran® HI-10

Manufacturer:  INEOS
Produced At:
  Korea / China
Product Category:  ABS
Product No:  Terluran HI-10
Product Quantity:  25KG / BAG
Product Features: 
Good Toughness,High Rigidity,High Strength,Low Temperature Impact Resistance,Medium Flow,Ultra High Impact Resistance

Terluran® HI-10

Acrylonitrile Butadiene Styrene
Product Description:
Terluran® HI-10 is an medium flow, injection molding grade with very high resistance to impact with excellent heat distortion and suitable for injection molding and extrusion.

FEATURES
  • High toughness

  • Very high impact

  • Medium flow

  • Great mechanical strength and rigidity

  • High impact at sub-zero temperatures


APPLICATIONS
  • Injection molding

  • Compounding

  • Appliance housings

  • Lawn & garden components requiring superior toughness


Features 
  • Good Toughness,High Rigidity,High Strength,Low Temperature Impact Resistance,Medium Flow,Ultra High Impact Resistance
Uses 
  • AppliancesCompoundingHousingsLawn and Garden Equipment 
Forms 
  • Pellets

Processing Method 
  • CompoundingExtrusionInjection Molding
Multi-Point Data 
  • Creep Modulus vs. Time (ISO 11403-1)

  • Isochronous Stress vs. Strain (ISO 11403-1)

  • Isothermal Stress vs. Strain (ISO 11403-1)

  • Secant Modulus vs. Strain (ISO 11403-1)

  • Specific Volume vs Temperature (ISO 11403-2)

  • Viscosity vs. Shear Rate (ISO 11403-2)

Physical
Nominal Value
Unit
Test Method
Density / Specific Gravity



--
1.03

ASTM D792
--
1.03
g/cm³
ISO 1183
Melt Mass-Flow Rate (MFR)


ASTM D1238
200°C/5.0 kg
0.10
g/10 min

220°C/10.0 kg
8.0
g/10 min

Melt Volume-Flow Rate (MVR)



230°C/3.8 kg
0.104
in³/10min
ASTM D1238
220°C/10.0 kg
0.336
in³/10min
ISO 1133
Molding Shrinkage



Flow
4.0E-3 to 7.0E-3
in/in
ASTM D955
--
0.40 to 0.70
%
ISO 294-4
Water Absorption



Saturation, 73°F
1.0
%
ASTM D570, ISO 62
Equilibrium, 73°F, 50% RH
0.21
%
ISO 62
Hardness
Nominal Value
Unit
Test Method
Rockwell Hardness (R-Scale)
95

ASTM D785
Ball Indentation Hardness
10700
psi
ISO 2039-1
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus



--
290000
psi
ASTM D638
--
276000
psi
ISO 527-2
Tensile Strength



Yield, 73°F
6240
psi
ASTM D638
Yield, 73°F
5510
psi
ISO 527-2
Tensile Strain



Yield, 73°F
2.8
%
ISO 527-2
Break
3.5
%
ASTM D638
Nominal Tensile Strain at Break (73°F)
9.0
%
ISO 527-2
Flexural Modulus
297000
psi
ASTM D790
Flexural Strength



--
9570
psi
ASTM D790
--
8120
psi
ISO 178
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength


ISO 179
-22°F
6.2
ft·lb/in²

73°F
17
ft·lb/in²

Charpy Unnotched Impact Strength


ISO 179
-22°F
67
ft·lb/in²

73°F
No Break


Notched Izod Impact



-22°F
2.2
ft·lb/in
ASTM D256
0°F
3.4
ft·lb/in
ASTM D256
73°F
8.4
ft·lb/in
ASTM D256
-22°F
6.7
ft·lb/in²
ISO 180/A
73°F
17
ft·lb/in²
ISO 180/A
Thermal
Nominal Value
Unit
Test Method
Deflection Temperature Under Load



66 psi, Unannealed
201
°F
ASTM D648
66 psi, Annealed
215
°F
ASTM D648
66 psi, Annealed 3
207
°F
ISO 75-2/B
264 psi, Unannealed
186
°F
ASTM D648
264 psi, Annealed
208
°F
ASTM D648
264 psi, Annealed 3
199
°F
ISO 75-2/A
Vicat Softening Temperature



--
217
°F
ISO 306/A50
--
194
°F
ISO 306/B50
CLTE - Flow
4.4E-5 to 6.1E-5
in/in/°F
ISO 11359-2
Thermal Conductivity
1.2
Btu·in/hr/ft²/°F
DIN 52612
Electrical
Nominal Value
Unit
Test Method
Volume Resistivity



--
> 1.0E+15
ohms·cm
ASTM D257
--
1.0E+15
ohms·cm
IEC 60093
Dielectric Constant



0.0394 in, 1 MHz
2.80

ASTM D150
100 Hz
2.90

IEC 60250
1 MHz
2.80

IEC 60250
Dissipation Factor


IEC 60250
100 Hz
5.4E-3


1 MHz
8.2E-3


Optical
Nominal Value
Unit
Test Method
Yellowness Index
15
YI
DIN 6167
Injection
Nominal Value
Unit

Drying Temperature
176
°F

Drying Time
2.0 to 4.0
hr

Processing (Melt) Temp
446 to 500
°F

Mold Temperature
86 to 176
°F

Injection Velocity
472
in/min



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields