Products

Makrolon® 3208

Makrolon® 3208

Manufacturer: Covestro
Produced At:
 Europe / China
Product Category: Polycarbonate
PC
Product No: Makrolon 3208 
Product Quantity: 25KG / BAG
Product Features: Biocompatible、Ethylene Oxide Sterilizable、High Viscosity、Steam Sterilizable

Makrolon® 3208

Polycarbonate
Product Description:
MVR (300°C/1.2 kg) 5.0 cm³/10 min; medical devices; suitable for ETO and steam sterilization at 121°C; biocompatible according to many ISO 10993-1 test requirements; high viscosity; injection molding - melt temperature 280 - 320°C; available in transparent and opaque colors

Features 
  • Biocompatible,Ethylene Oxide Sterilizable,

  • High Viscosity,Steam Sterilizable 

Uses 
  • Medical Devices,Medical/Healthcare Applications 
Agency Ratings 
  • ISO 10993-Part 1

RoHS Compliance 
  • RoHS Compliant

Appearance 
  • Clear/Transparent,Colors Available,Opaque
Processing Method 
  • Injection Molding

Multi-Point Data 
  • Creep Modulus vs. Time (ISO 11403-1)

  • Isochronous Stress vs. Strain (ISO 11403-1)

  • Isothermal Stress vs. Strain (ISO 11403-1)

  • Secant Modulus vs. Strain (ISO 11403-1)

  • Shear Modulus vs. Temperature (ISO 11403-1)

  • Specific Volume vs Temperature (ISO 11403-2)

  • Viscosity vs. Shear Rate (ISO 11403-2)

Physical
Nominal Value
Unit
Test Method
Density (73°F)
1.20
g/cm³
ISO 1183
Apparent (Bulk) Density 3
0.66
g/cm³
ISO 60
Melt Mass-Flow Rate (MFR) (300°C/1.2 kg)
5.5
g/10 min
ISO 1133
Melt Volume-Flow Rate (MVR) (300°C/1.2 kg)
0.305
in³/10min
ISO 1133
Molding Shrinkage



Across Flow
0.60 to 0.80
%
ISO 2577
Flow
0.60 to 0.80
%
ISO 2577
Across Flow : 536°F, 0.0787 in 4
0.75
%
ISO 294-4
Flow : 0.0787 in 4
0.70
%
ISO 294-4
Water Absorption


ISO 62
Saturation, 73°F
0.30
%

Equilibrium, 73°F, 50% RH
0.12
%

Hardness
Nominal Value
Unit
Test Method
Ball Indentation Hardness
16100
psi
ISO 2039-1
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus (73°F)
341000
psi
ISO 527-2/1
Tensile Stress


ISO 527-2/50
Yield, 73°F
9430
psi

Break, 73°F
10900
psi

Tensile Strain


ISO 527-2/50
Yield, 73°F
6.3
%

Break, 73°F
120
%

Nominal Tensile Strain at Break (73°F)
> 50
%
ISO 527-2/50
Tensile Creep Modulus


ISO 899-1
1 hr
319000
psi

1000 hr
276000
psi

Flexural Modulus 5 (73°F)
341000
psi
ISO 178
Flexural Stress 5


ISO 178
73°F
13800
psi

3.5% Strain, 73°F
10400
psi

Flexural Strain at Flexural Strength 6 (73°F)
7.2
%
ISO 178
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength 7, 8


ISO 7391
-22°F, Complete Break
8.6
ft·lb/in²

73°F, Partial Break
38
ft·lb/in²

Charpy Unnotched Impact Strength


ISO 179/1eU
-76°F
No Break


-22°F
No Break


73°F
No Break


Notched Izod Impact Strength 9, 8


ISO 7391
-22°F, Complete Break
9.5
ft·lb/in²

73°F
36
ft·lb/in²

Multi-Axial Instrumented Impact Energy


ISO 6603-2
-22°F
55.3
ft·lb

73°F
47.9
ft·lb

Multi-Axial Instrumented Impact Peak Force


ISO 6603-2
-22°F
1510
lbf

73°F
1300
lbf

Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature



66 psi, Unannealed
288
°F
ISO 75-2/B
264 psi, Unannealed
266
°F
ISO 75-2/A
Glass Transition Temperature 10
302
°F
ISO 11357-2
Vicat Softening Temperature



--
302
°F
ISO 306/B50
--
304
°F
ISO 306/B120
Ball Pressure Test (286°F)
Pass

IEC 60695-10-2
CLTE


ISO 11359-2
Flow : 73 to 131°F
3.6E-5
in/in/°F

Transverse : 73 to 131°F
3.6E-5
in/in/°F

Thermal Conductivity 11 (73°F)
1.4
Btu·in/hr/ft²/°F
ISO 8302
Flammability
Nominal Value
Unit
Test Method
Oxygen Index 12
27
%
ISO 4589-2
Flash Ignition Temperature
896
°F
ASTM D1929
Self Ignition Temperature
1022
°F
ASTM D1929
Optical
Nominal Value
Unit
Test Method
Refractive Index 13
1.587

ISO 489
Transmittance


ISO 13468-2
39.4 mil
89.0
%

78.7 mil
89.0
%

118 mil
88.0
%

157 mil
87.0
%

Haze (118 mil)
< 0.80
%
ISO 14782
Additional Information
Nominal Value

Test Method
ISO Shortname
PC,M,(,,)-05-9

ISO 7391


Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation
展开