Products

Makrolon® 1952

Makrolon® 1952

Manufacturer: Covestro
Produced At:
 Europe / China
Product Category: Polycarbonate
PC
Product No: Makrolon 1952 
Product Quantity: 25KG / BAG
Product Features: Good Mold Release,Medium Viscosity

Makrolon® 1952

Polycarbonate
Product Description:
MVR (300 °C/1.2 kg) 10 cm³/10 min; flame retardant; UL 94V-0/2.3 mm; medium viscosity; UV stabilized; easy release; injection molding - melt temperature 280 - 320 °C; available in translucent and opaque colors; LCD notebook cover

Additive 
  • Flame Retardant,UV Stabilizer 
Features 
  • Flame Retardant,Good Mold Release,Medium Viscosity
Uses 
  • Computer Components

RoHS Compliance 
  • RoHS Compliant

Appearance 
  • Colors Available,Opaque,Translucent
Processing Method 
  • Injection Molding

Physical
Nominal Value
Unit
Test Method
Density (73°F)
1.20
g/cm³
ISO 1183
Apparent (Bulk) Density 2
0.64
g/cm³
ISO 60
Melt Mass-Flow Rate (MFR) (300°C/1.2 kg)
10
g/10 min
ISO 1133
Melt Volume-Flow Rate (MVR) (300°C/1.2 kg)
0.610
in³/10min
ISO 1133
Molding Shrinkage



Across Flow
0.60 to 0.80
%
ISO 2577
Flow
0.60 to 0.80
%
ISO 2577
Across Flow : 0.0787 in 3
0.70
%
ISO 294-4
Flow : 0.0787 in 3
0.65
%
ISO 294-4
Water Absorption


ISO 62
Saturation, 73°F
0.30
%

Equilibrium, 73°F, 50% RH
0.12
%

Hardness
Nominal Value
Unit
Test Method
Ball Indentation Hardness
16700
psi
ISO 2039-1
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus (73°F)
348000
psi
ISO 527-2/1
Tensile Stress


ISO 527-2/50
Yield, 73°F
9570
psi

Break, 73°F
10200
psi

Tensile Strain


ISO 527-2/50
Yield, 73°F
6.1
%

Break, 73°F
130
%

Nominal Tensile Strain at Break (73°F)
> 50
%
ISO 527-2/50
Tensile Creep Modulus


ISO 899-1
1 hr
319000
psi

1000 hr
276000
psi

Flexural Modulus 4 (73°F)
348000
psi
ISO 178
Flexural Stress 4


ISO 178
73°F
14400
psi

3.5% Strain, 73°F
10900
psi

Flexural Strain at Flexural Strength 5 (73°F)
7.0
%
ISO 178
Films
Nominal Value
Unit
Test Method
Water Vapor Transmission Rate (73°F, 85% RH, 3.9 mil)
0.97
g/100 in²/24 hr
ISO 15106-1
Gas Permeation


ISO 2556
Carbon Dioxide : 73°F, 1.0 mil
16900
cm³/m²/bar/24 hr

Carbon Dioxide : 73°F, 3.9 mil
3800
cm³/m²/bar/24 hr

Nitrogen : 73°F, 1.0 mil
510
cm³/m²/bar/24 hr

Nitrogen : 73°F, 3.9 mil
120
cm³/m²/bar/24 hr

Oxygen : 73°F, 1.0 mil
2760
cm³/m²/bar/24 hr

Oxygen : 73°F, 3.9 mil
650
cm³/m²/bar/24 hr

Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength 6


ISO 7391
-22°F, Complete Break
6.7
ft·lb/in²

73°F, Partial Break
33
ft·lb/in²

Charpy Unnotched Impact Strength


ISO 179/1eU
-22°F
No Break


73°F
No Break


Notched Izod Impact Strength 7


ISO 7391
-22°F, Complete Break
5.7
ft·lb/in²

73°F, Partial Break
31
ft·lb/in²

Multi-Axial Instrumented Impact Energy


ISO 6603-2
-22°F
47.9
ft·lb

73°F
44.3
ft·lb

Multi-Axial Instrumented Impact Peak Force


ISO 6603-2
-22°F
1420
lbf

73°F
1210
lbf

Thermal
Nominal Value
Unit
Test Method
Heat Deflection Temperature



66 psi, Unannealed
277
°F
ISO 75-2/B
264 psi, Unannealed
255
°F
ISO 75-2/A
Glass Transition Temperature 8
291
°F
ISO 11357-2
Vicat Softening Temperature



--
289
°F
ISO 306/B50
--
291
°F
ISO 306/B120
Ball Pressure Test (275°F)
Pass

IEC 60695-10-2
CLTE


ISO 11359-2
Flow : 73 to 131°F
3.6E-5
in/in/°F

Transverse : 73 to 131°F
3.6E-5
in/in/°F

Thermal Conductivity 9 (73°F)
1.4
Btu·in/hr/ft²/°F
ISO 8302


Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields