Elastollan® S60DN
Thermoplastic Polyurethane Elastomer (Polyester)
Product Description:
Elastollan® S60DN exhibits excellent abrasion resistance, toughness, good heat, oil, fuel, and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® S60DN is supplied uncolored in diced form.
Appearance | Colorless |
Processing Method | Extrusion、Injection Molding |
Density / Specific Gravity | 1.25 |
| ASTM D792 |
Durometer Hardness (Shore D) | 60 |
| ASTM D2240 |
Tensile Modulus (Injection Molded) | 27000 | psi | ASTM D412 |
Flexural Modulus (Injection Molded) | 22000 | psi | ASTM D790 |
Taber Abrasion Resistance | 50.0 | mg | ASTM D1044 |
Abrasion - DIN | 25 | mm³ | DIN 53516 |
Tensile Stress |
|
| ASTM D412 |
100% Strain | 3200 | psi |
|
300% Strain | 6500 | psi |
|
Tensile Strength | 7300 | psi | ASTM D412 |
Tensile Elongation (Break) | 400 | % | ASTM D412 |
Tear Strength 2 | 1300 | lbf/in | ASTM D624 |
Compression Set |
|
| ASTM D395B |
73°F, 22 hr | 40 | % |
|
158°F, 22 hr | 50 | % |
|
Glass Transition Temperature | 17.6 | °F | Internal Method |
Vicat Softening Temperature | 293 | °F | ASTM D1525 |
Softening Point - DMA | 297 | °F | Internal Method |
Drying Temperature | 230 to 248 | °F |
|
Drying Time | 2.0 to 3.0 | hr |
|
Suggested Max Moisture | 0.030 | % |
|
Rear Temperature | 410 to 446 | °F |
|
Middle Temperature | 410 to 446 | °F |
|
Front Temperature | 410 to 446 | °F |
|
Nozzle Temperature | 428 to 464 | °F |
|