Elastollan® C95A10
Thermoplastic Polyurethane Elastomer (Polyester)
Product Description:
Elastollan® C95A exhibits excellent abrasion resistance and toughness, good hydrolytic stability, good heat, oil, fuel and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® C95A is supplied uncolored in diced or pelletized form.
Appearance | |
Processing Method | ExtrusionInjection Molding |
Density / Specific Gravity | 1.21 |
| ASTM D792 |
Melt Mass-Flow Rate (MFR) (215°C/21.6 kg) | 50 to 110 | g/10 min | ASTM D1238 |
Durometer Hardness (Shore A) | 95 |
| ASTM D2240 |
Tensile Modulus (Injection Molded) | 9000 | psi | ASTM D412 |
Flexural Modulus (Injection Molded) | 11000 | psi | ASTM D790 |
Taber Abrasion Resistance | 30.0 | mg | ASTM D1044 |
Abrasion - DIN | 25 | mm³ | DIN 53516 |
Tensile Stress |
|
| ASTM D412 |
100% Strain | 2200 | psi |
|
300% Strain | 5300 | psi |
|
Tensile Strength | 6700 | psi | ASTM D412 |
Tensile Elongation (Break) | 440 | % | ASTM D412 |
Tear Strength 2 | 870 | lbf/in | ASTM D624 |
Compression Set |
|
| ASTM D395B |
73°F, 22 hr | 30 | % |
|
158°F, 22 hr | 45 | % |
|
Glass Transition Temperature | -32.8 | °F | Internal Method |
Vicat Softening Temperature | 275 | °F | ASTM D1525 |
Softening Point - DMA | 253 | °F | Internal Method |
Drying Temperature | 230 to 248 | °F |
|
Drying Time | 2.0 to 3.0 | hr |
|
Suggested Max Moisture | 0.030 | % |
|
Rear Temperature | 374 to 428 | °F |
|
Middle Temperature | 374 to 428 | °F |
|
Front Temperature | 374 to 428 | °F |
|
Nozzle Temperature | 410 to 437 | °F |
|
Drying Temperature | 230 to 248 | °F |
|
Drying Time | 2.0 to 3.0 | hr |
|
Cylinder Zone 1 Temp. | 338 to 410 | °F |
|
Cylinder Zone 3 Temp. | 338 to 410 | °F |
|
Cylinder Zone 5 Temp. | 338 to 410 | °F |
|
Adapter Temperature | 392 to 428 | °F |
|
Die Temperature | 383 to 419 | °F |
|