Products

Elastollan® 1154D

Elastollan® 1154D

Manufacturer: BASF
Produced At:
 Europe / China
Product Category: TPU
Product No: Elastollan 1154D
Product Quantity: 25KG / BAG
Product Features:
 Abrasion ResistantFood Contact AcceptableFungus ResistantGood Tear StrengthGood ToughnessHydrolytically StableLow Temperature Flexibility

Elastollan® 1154D

Thermoplastic Polyurethane Elastomer (Polyether)
Product Description:
Elastollan® 1154D exhibits excellent abrasion resistance, toughness, transparency, very good low temperature flexibility, hydrolytic stability and fungus resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® 1154D conforms to the FDA food contact regulations as described in book 21, section 177.2600 for wet food contact applications. Elastollan® 1154D also has NSF Standard 61 "Water Contact Material" certification. Elastollan® 1154D is supplied uncolored in diced form.

Agency Ratings 
FDA 21 CFR 177.2600/NSF STD-61 
Appearance 
  • Clear/Transparent

Processing Method 
Extrusion/Injection Molding 
Physical
Nominal Value

Test Method
Density / Specific Gravity
1.16

ASTM D792
Hardness
Nominal Value

Test Method
Durometer Hardness (Shore D)
54

ASTM D2240
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus (0.0866 in, Injection Molded)
22000
psi
ASTM D412
Flexural Modulus (0.0866 in, Injection Molded)
24000
psi
ASTM D790
Taber Abrasion Resistance
60.0
mg
ASTM D1044
Abrasion - DIN
30
mm³
DIN 53516
Elastomers
Nominal Value
Unit
Test Method
Tensile Stress


ASTM D412
100% Strain, 0.0866 in
3800
psi

300% Strain, 0.0866 in
6600
psi

Tensile Strength (0.0866 in)
7000
psi
ASTM D412
Tensile Elongation (Break, 0.0866 in)
410
%
ASTM D412
Tear Strength 2 (0.0866 in)
1200
lbf/in
ASTM D624
Compression Set


ASTM D395B
73°F, 22 hr
40
%

158°F, 22 hr
50
%

Thermal
Nominal Value
Unit
Test Method
Glass Transition Temperature
3.20
°F
Internal Method
Vicat Softening Temperature
280
°F
ASTM D1525
Softening Point - DMA
261
°F
Internal Method
Injection
Nominal Value
Unit

Drying Temperature
230 to 248
°F

Drying Time
2.0 to 3.0
hr

Suggested Max Moisture
0.030
%

Rear Temperature
410 to 446
°F

Middle Temperature
410 to 446
°F

Front Temperature
410 to 446
°F

Nozzle Temperature
428 to 464
°F



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields


Consultation
展开